DAMPING CAPACITY OF FE-CR ALLOYS

被引:23
作者
MASUMOTO, H
SAWAYA, S
HINAI, M
机构
来源
TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS | 1979年 / 20卷 / 08期
关键词
D O I
10.2320/matertrans1960.20.409
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
In alloys slow-cooled after heating at 800 similar 1200 degree C, the value of Q** minus **1 which shows two maxima at concentrations of 5 and 15% Cr increases with increasing heating temperature. An Fe-15% Cr alloy exhibits the highest Q** minus **1 value of 68 multiplied by 10** minus **3 ( gamma //m equals 80 multiplied by 10** minus **6) when slow-cooled after heating at 1200 degree C. The high value is due to the effect of magnetomechanical hysteresis.
引用
收藏
页码:409 / 413
页数:5
相关论文
共 15 条
  • [1] Some magneto-elastic torsion tests
    Becker, R.
    Kornetzki, M.
    [J]. ZEITSCHRIFT FUR PHYSIK, 1934, 88 (9-10): : 634 - 646
  • [2] COCHARDT AW, 1953, J APPL MECH-T ASME, V20, P196
  • [3] COCHARDT AW, 1955, T ASM, V47, P440
  • [4] COCHARDT AW, 1958, MAGNETIC PROPERTIES, P251
  • [5] Hansen M., 1958, J ELECTROCHEM SOC, DOI DOI 10.1149/1.2428700
  • [6] IMAI Y, 1966, J JPN I MET, V30, P284
  • [7] APPARATUS FOR CONTINUOUS RECORDING OF INTERNAL FRICTION
    KOFSTAD, P
    BUTERA, RA
    CRAIG, RS
    [J]. REVIEW OF SCIENTIFIC INSTRUMENTS, 1962, 33 (08) : 850 - &
  • [8] KOIWA M, 1966, SCI REP RES TOHOKU A, VS 18, P344
  • [9] DAMPING CAPACITY OF GENTALLOY IN FE-CO ALLOYS
    MASUMOTO, H
    SAWAYA, S
    HINAI, M
    [J]. TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1978, 19 (06): : 312 - 316
  • [10] DAMPING CAPACITY OF FE-MO ALLOYS
    MASUMOTO, H
    SAWAYA, S
    HINAI, M
    [J]. TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1977, 18 (08): : 581 - 584