- [31] DEVELOPMENT OF HIGH-STRENGTH 12CR-1MO-1W-V-NB STEEL TUBE FOR BOILER .1. EFFECTS OF CHEMICAL-COMPOSITIONS AND HEAT-TREATMENT CONDITION ON CREEP-RUPTURE STRENGTH AND MICROSTRUCTURE OF 12-PERCENT-CR STEELS FOR BOILER TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 26 (12) : B371 - B371
- [32] Welding residual stress effect of the fatigue strength at dissimilar material weld between Alloy617 and 12Cr steel INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2018, 32 (19):
- [35] SEGREGATION OF SULFUR AND NITROGEN AT THE SURFACE OF A 12-PERCENT CR STEEL (Z20-CDV-12.1) FOLLOWING CONTINUOUS CO2-LASER FUSION MEMOIRES ET ETUDES SCIENTIFIQUES DE LA REVUE DE METALLURGIE, 1988, 85 (09): : 459 - 459
- [36] INDUCTION ASSISTED HYBRID FRICTION STIR WELDING OF DISSIMILAR MATERIALS AA5052 ALUMINIUM ALLOY AND X12Cr13 STAINLESS STEEL ADVANCES IN MATERIALS SCIENCE, 2021, 21 (03): : 17 - 30