The removal of internal stress in 70 : 30 brass by low temperature annealing.

被引:0
|
作者
Moore, H
Beckinsale, S
机构
来源
JOURNAL OF THE INSTITUTE OF METALS | 1920年 / 23卷
关键词
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
引用
收藏
页码:225 / 245
页数:23
相关论文
共 50 条
  • [31] Optimization of Annealing Temperature for PVDF-TrFE (70:30 mol %) Thin Film
    Wahid, Mohamad Hafiz Mohd
    Dahan, Rozana Mohd
    Sa'ad, Siti Zaleha
    Arshad, Adillah Nurashikin
    Sarip, Muhamad Naiman
    Mahmood, Mohamad Rusop
    Abd Majid, Wan Haliza
    ADVANCED MATERIALS ENGINEERING AND TECHNOLOGY, 2012, 626 : 721 - +
  • [32] EFFECTS OF SMALL SURFACE CRACKS ON DUCTILITY LOSS IN LOW-CYCLE FATIGUE OF 70/30 BRASS
    MURAKAMI, Y
    MAKABE, C
    NISITANI, H
    JOURNAL OF TESTING AND EVALUATION, 1989, 17 (01) : 20 - 27
  • [33] LOW-TEMPERATURE ELECTRON-IRRADIATION OF ALPHA-BRASS - DEFECT ANNEALING AND ASSIGNMENT
    DAMASK, AC
    GILBERT, J
    HERMAN, H
    RADIATION EFFECTS AND DEFECTS IN SOLIDS, 1975, 26 (1-2): : 89 - 94
  • [34] The inhibition of the stress corrosion cracking of 70/30 brass in nitrite solution with additions of alloying arsenic and arsenic anions
    Luo, X
    Yu, J
    CORROSION SCIENCE, 1996, 38 (05) : 767 - 780
  • [35] DEFORMATION-BEHAVIOR OF A 70/30 ALPHA-BRASS IN PLANE-STRESS PLANE-STRAIN
    SUNDARAM, PA
    RODRIGUEZ, D
    SANTIAGO, S
    SCRIPTA METALLURGICA ET MATERIALIA, 1994, 30 (01): : 95 - 100
  • [36] THE EFFECT OF LOW-TEMPERATURE ANNEALING ON THE INDENTATION HARDNESS OF COLD-WORKED ALPHA-BRASS
    BAIRD, C
    JENNINGS, PH
    JOURNAL OF THE INSTITUTE OF METALS, 1961, 89 (06): : 191 - 192
  • [37] Influence of annealing temperature on the structural and optical properties of As30Te70 thin films
    Abd-Elnaiem, A. M.
    Mohamed, M.
    Hassan, R. M.
    Abu-Sehly, A. A.
    Abdel-Rahim, M. A.
    Hafiz, M. M.
    MATERIALS SCIENCE-POLAND, 2017, 35 (02): : 335 - 345
  • [38] THE INTERMEDIATE TEMPERATURE DUCTILITY MINIMUM IN 70-PERCENT-CU AND 30-PERCENT-ZN ALPHA-BRASS
    WAGH, AS
    EZEGBUNAM, LN
    SCRIPTA METALLURGICA, 1984, 18 (09): : 933 - 937
  • [39] The influence of low temperature pre-annealing on the defect removal and the reduction of junction depth in excimer laser annealing
    Baek, S
    Jang, T
    Hwang, H
    SILICON FRONT-END JUNCTION FORMATION TECHNOLOGIES, 2002, 717 : 57 - 61
  • [40] Further studies in season-cracking and its prevention. The removal of internal stress in 60 : 40 brass.
    Beckinsale, S
    JOURNAL OF THE INSTITUTE OF METALS, 1923, 29 : 285 - 296