NATURAL RUBBER-HDPE BLENDS WITH LIQUID NATURAL-RUBBER AS A COMPATIBILIZER .1. THERMAL AND MECHANICAL-PROPERTIES

被引:33
作者
AHMAD, S [1 ]
ABDULLAH, I [1 ]
SULAIMAN, CS [1 ]
KOHJIYA, S [1 ]
YOON, JR [1 ]
机构
[1] KYOTO INST TECHNOL,DEPT MAT SCI,KYOTO 606,JAPAN
关键词
D O I
10.1002/app.1994.070510801
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The measurement of physical properties of thermoplastic natural rubber (TPNR) of NR-HDPE blends have been made at various compositions of high-density polyethylene (HDPE). The tensile properties and hardness of TPNR improve significantly with the addition of liquid natural rubber (LNR) to the blend. The degree of cross-linking also increases with increasing amount of LNR added. The LNR with molecular weight (M(w)) of 50,000 and reactive terminals promotes cross-linking within the rubber phase and grafting of the polyethylene chains onto the rubber matrix system. The maximum stress and strain of the blends measured are about 7.5 MPa and 1000%, respectively. Dynamic mechanical analysis results indicate a single T-g on a tan delta trace at about -50 and -55 degrees C for the two types of blends, respectively. (C) 1994 John Wiley & Sons, Inc.
引用
收藏
页码:1357 / 1363
页数:7
相关论文
共 8 条
[1]  
ABDULLAH I, 1992, J MATER FORUM, P16
[2]  
CAMPBELL DS, 1988, NR TECHNOL, V9, P21
[3]  
Elliott D. J., 1981, NR TECHNOL, V12, P59
[4]   RUBBER TOUGHENING OF POLYSTYRENE THROUGH REACTIVE BLENDING [J].
FOWLER, MW ;
BAKER, WE .
POLYMER ENGINEERING AND SCIENCE, 1988, 28 (21) :1427-1433
[5]   THE RUBBER PARTICLE-SIZE DEPENDENCE OF CRAZING IN POLYPROPYLENE [J].
JANG, BZ ;
UHLMANN, DR ;
VANDERSANDE, JB .
POLYMER ENGINEERING AND SCIENCE, 1985, 25 (10) :643-651
[6]  
QIN C, 1990, J RUBBER CHEM TECHNO, V63, P1
[7]  
THINKER AJ, 1984, POLYM COMMUN, V25, P325
[8]  
1987, DATA BOOK THERMAL PR