Effects of Specimen Size and Side-groove on the Results of J-R Fracture Toughness Test for LBB Evaluation

被引:4
作者
Kim, Jin Weon [1 ]
Choi, Myung Rak [1 ]
Oh, Young Jin [2 ]
Park, Heung Bae [2 ]
Kim, Kyung Su [2 ]
机构
[1] Chosun Univ, Dept Nucl Engn, Gwangju, South Korea
[2] KEPCO E&C, Elect Technol Res Inst, Gimcheon, South Korea
关键词
J-R Fracture Toughness Test; Specimen Size; SA508 Gr. 1a Piping Material; LBB Evaluation;
D O I
10.3795/KSME-A.2015.39.7.729
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this study, the effects of specimen size and side-groove on the results of the J-R test for leak-before-break (LBB) evaluation were investigated. A series of J-R tests were conducted at both RT and 316 degrees C, using three different sizes of compact tension (CT) specimens machined from SA508 Gr.1a piping material: 12.7 mm-thick 1T-CT, 25.4 mm-thick 1T-CT, and 25.4 mm-thick 2T-CT with and without side-groove. The results showed that side-grooving reduced the J-R curve for all specimens and the effect of side-grooving was more significant at 316 degrees C than at RT. As the thickness of the specimens decreased and the width of the specimens increased, the J-R curve slightly decreased at RT but it increased at 316 degrees C. However, the variation in the J-R curve of SA508 Gr.1a with the thickness and width of CT specimen was insignificant.
引用
收藏
页码:729 / 736
页数:8
相关论文
共 15 条
  • [1] [Anonymous], 2009, ASTME8E8M09
  • [2] ASTM E1820-08a, 2009, ASTM INT, P1
  • [3] Dietzel W., 1986, Materialpruefung, V28, P368
  • [4] EPRI, 1989, NSAC141 EPRI
  • [5] IMAI Y, 1982, ENG FRACT MECH, V16, P659, DOI 10.1016/0013-7944(82)90019-4
  • [6] *ISO, 2002, ISO12135
  • [7] JOHNSON HH, 1965, MATER RES STANDARD, V5, P442
  • [8] Influences of the dynamic strain aging on the J-R fracture characteristics of the ferritic steels for reactor coolant piping system
    Kim, KC
    Kim, JT
    Suk, JI
    Sung, UH
    Kwon, HK
    [J]. NUCLEAR ENGINEERING AND DESIGN, 2004, 228 (1-3) : 151 - 159
  • [9] J-R fracture properties of SA508-1a ferritic steels and SA312-TP347 austenitic steels for pressurized water reactor's (PWR) primary coolant piping
    Lee, BS
    Oh, YJ
    Yoon, JH
    Kuk, IH
    Hong, JH
    [J]. NUCLEAR ENGINEERING AND DESIGN, 2000, 199 (1-2) : 113 - 123
  • [10] Specimen size effects on fracture toughness of JLF-1 reduced-activation ferritic steel
    Ono, H
    Kasada, R
    Kimura, A
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2004, 329 : 1117 - 1121