THE CORROSION BEHAVIOR OF NI-AL ALLOYS AND NI-NB-AL ALLOYS IN A H2/H2O/H2S GAS-MIXTURE

被引:3
|
作者
HE, YR [1 ]
DOUGLASS, DL [1 ]
机构
[1] UNIV CALIF LOS ANGELES,DEPT MAT SCI & ENGN,LOS ANGELES,CA 90024
来源
OXIDATION OF METALS | 1993年 / 40卷 / 3-4期
关键词
MIXED GAS; NI-NB-AL ALLOYS; NI-AL ALLOYS; AL2O3; AL2S3; NINB3S6; NB3S4;
D O I
10.1007/BF00664497
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The corrosion behavior of two Ni-Al alloys and four Ni-Nb-Al alloys was studied over the temperature range of 600-degrees-C to 1000-degrees-C in a mixed-gas of H-2/H2O/H2S. The parabolic law was generally followed, although linear kinetics were also observed. Multiple-stage kinetics were observed for the Ni-Al alloys. Generally, the scales formed on Ni-13.5Al and Ni-Nb-Al alloys were multilayered, with an outer layer of nickel sulfide with or without pure Ni particles and a complex inner scale. The outer scale became porous and discontinuous with increasing temperature. Very thin scales formed on Ni-31Al. The reduction in corrosion rate with increasing Al content is ascribed to the formation of Al2O3 and Al2S3 in the scale. Platinum markers were found at the interface between the outer and inner scales.
引用
收藏
页码:337 / 371
页数:35
相关论文
共 50 条
  • [31] The high-temperature corrosion of Fe-28Al base alloys containing Cr and Y additions in H2/H2S/H2O mixed gases
    Kai, W
    Chang, MT
    Liu, CD
    Chiang, DL
    Chu, JP
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 329 : 734 - 744
  • [32] HIGH-TEMPERATURE CORROSION OF FE-NI-CR, FE-CR-AL AND FE-NI-CR-AL ALLOYS IN CONTROLLED H2/H2O/CH4 ATMOSPHERES
    LOUDJANI, MK
    PIVIN, JC
    HUNTZ, AM
    DAVIDSON, JH
    CORROSION SCIENCE, 1988, 28 (11) : 1075 - 1088
  • [33] INVESTIGATIONS OF HIGH-TEMPERATURE SULFIDIZATION OF STEELS IN H2/H2S AND H2/H2S/H2O GAS-MIXTURES
    GROSSER, W
    MEDER, D
    AUER, W
    KAESCHE, H
    WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1992, 43 (04): : 145 - 153
  • [35] The Corrosion Behavior about two Ni-based alloys in CO2 / H2S Environments
    Zhao, XueHui
    Bai, ZhenQuan
    Lin, Kai
    Han, Yan
    NEW MATERIALS AND ADVANCED MATERIALS, PTS 1 AND 2, 2011, 152-153 : 1624 - 1631
  • [36] H2 generation from H2S decomposition on Al
    Hai, Pengqi
    Wu, Chao
    Ding, Xiangdong
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2024, 67 : 1097 - 1105
  • [37] The Corrosion of Titanium Aluminides in H2/H2S/H2O Atmospheres at 800–1000°C
    W. Kai
    M. T. Chang
    C. Y. Bai
    Oxidation of Metals, 2001, 56 : 191 - 214
  • [38] SINTERING OF NI-AL203 CATALYSTS IN H2/H2O ATMOSPHERE - INFLUENCE ON METHANIZATION ACTIVITY
    BARTHOLOMEW, CH
    PANNELL, RB
    ERDOL & KOHLE ERDGAS PETROCHEMIE, 1979, 32 (03): : 140 - 140
  • [39] Corrosion of Fe-(4.8, 9.2, 14.3) Wt%Al alloys at 700 and 800 °C in N2/H2O/H2S gases
    Min Jung Kim
    Dong Bok Lee
    Metals and Materials International, 2013, 19 : 975 - 982
  • [40] Corrosion Behaviors of Ni–Cr Alloys in O2, H2O and H2O + O2 Gases at 700°C and the Effect of Temperature
    Jiarui Chen
    Chengyang Jiang
    Jianqiang Zhang
    High Temperature Corrosion of Materials, 2023, 100 : 775 - 789