摘要
The rate of the decarburization of carbon-saturated liquid iron by H2O gas between 1673 and 1873 K has been studied under conditions in which the effect of mass transfer is negligible, or a reasonable correction for its effect can be made. The rate was measured for water vapor pressures in the range 0.002 to 0.3 atm and sulfur contents in the metal from 0.005 to 0.5 mass pct. The measured rates are consistent with the rate-controlling reaction being the dissociation of H2O on the surface. Sulfur was found to significantly decrease the rate, and the residual rate phenomenon was observed at high sulfur content. The rate constant for the dissociation of H2O on liquid iron is given by k = k-degrees/1 + K(S)a(S) + k(r) where k-degrees, k(r), K(S), and a(S) are the rate constant for pure iron, residual rate constant, the adsorption coefficient of sulfur, and the activity of sulfur in the metal relative to 1 mass pct in carbon-saturated liquid iron, respectively. The rate constants and adsorption coefficient were determined to be log k-degrees = -4860/T + 0.57 (mol/cm2 s atm) log k(r) = -5350/T - 1.03 (mol/cm2 s atm) log K(S) = 3870/T + 0.51
引用
收藏
页码:245 / 253
页数:9
相关论文
共 50 条
  • [1] Kinetics of the reaction of H2O gas with liquid iron
    Nagasaka, T.
    Fruehan, R.J.
    Metallurgical transactions. B, Process metallurgy, 1994, 25 (02): : 245 - 253
  • [2] ON THE INTERFACIAL KINETICS OF THE REACTION OF CO2 WITH LIQUID-IRON
    HUA, CH
    PARLEE, NAD
    METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1983, 14 (03): : 504 - 506
  • [3] KINETICS OF REACTION BETWEEN NITROGEN AND LIQUID-IRON
    VITOL, EN
    ORLOVA, KB
    RUSSIAN METALLURGY, 1973, 1974 (03): : 52 - 57
  • [4] DECARBURIZATION RATES OF LIQUID-IRON BY H2O IN HIGH SULFUR CONCENTRATION RANGE
    SASAKI, Y
    BELTON, GR
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 26 (07) : 611 - 613
  • [5] THE KINETICS OF NITROGEN REACTION WITH LIQUID-IRON AND IRON-ALLOYS
    GLAWS, PC
    FRUEHAN, RJ
    JOURNAL OF METALS, 1984, 36 (12): : 23 - 23
  • [6] KINETICS OF NITROGEN DESORPTION REACTION OF LIQUID-IRON AND STEEL
    NARITA, K
    KOYAMA, S
    MAKINO, T
    OKAMURA, M
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1972, 12 (06) : 444 - 453
  • [7] KINETICS OF EVAPORATION OF LIQUID-IRON
    GRIGORYA.VA
    ALEEV, RA
    KOCHETOV, AI
    PRYANISH.MI
    STEEL IN THE USSR, 1973, 3 (03): : 199 - 200
  • [8] KINETICS OF OXYGEN DISSOLUTION IN LIQUID-IRON AND LIQUID-IRON ALLOY DROPLETS
    GREENBERG, LA
    MCLEAN, A
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1974, 14 (06) : 395 - 403
  • [9] KINETICS OF THE RAPID GAS PHASE REACTION BETWEEN NO, NO2, AND H2O
    WAYNE, LG
    YOST, DM
    JOURNAL OF CHEMICAL PHYSICS, 1951, 19 (01): : 41 - 47
  • [10] Is H2O a liquid, or water a gas?
    Soames, Scott
    PHILOSOPHY AND PHENOMENOLOGICAL RESEARCH, 2006, 72 (03) : 635 - 639