HYDROGEN BUBBLES IN EMBRITTLED AL-ZN-MG ALLOYS

被引:65
作者
SCAMANS, GM
机构
关键词
D O I
10.1007/BF00739268
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
引用
收藏
页码:27 / 36