THE GENERATION AND CHARACTERIZATION OF SILICON-CARBIDE WHISKERS (FIBERS) FOR INHALATION TOXICOLOGY STUDIES

被引:0
|
作者
CRAIG, DK
LAPIN, CA
BUTTERFIELD, GE
机构
[1] ARCO,LOS ANGELES,CA 90071
[2] SAVANNAH RIVER LABS,AIKEN,SC 29802
[3] STATE MICHIGAN DEPT NAT RESOURCES,LANSING,MI 48909
来源
关键词
D O I
暂无
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Atmospheres of silicon carbide whiskers (wh) were required for a repeated dose lung deposition study and a subchronic inhalation toxicity study, each involving exposure to three concentrations of whiskers for 6 hr/day, 5 days/week for 1 or 13 weeks. Target concentrations were 0, 500, 1500, and 7500 wh/cc. By using the mean fiber length (10 mum), diameter (0.555 mum), and density (3.2 g/cc) of the bulk material, target mass concentrations were approximately 0, 4, 12, and 60 mg/m3. The Pitt III generator, developed for cotton fiber dispersion at the University of Pittsburgh, was selected. This instrument consists of a vertical 18-in. long cylinder, which is closed at each end with rubber dams and coupled at the base to a loudspeaker. The sonic energy from the loudspeaker fluidizes the test material and the whiskers in the air column are carried out with the exhaust air. The output of the Pitt III generator was altered by changing the sound energy input, the rate of introduction of the test material into the fluidizing cylinder, or the airflow through the cylinder. Separate generation systems were used for each inhalation chamber. Chamber atmospheres were characterized gravimetrically and samples were analyzed by scanning electron microscopy. Mean mass and number concentrations for the subchronic study were 0.09, 3.93, 10.7, and 60.5 mg/m3 and 0, 630, 1746, and 7276 wh/cc, respectively. Weighted mean values for whisker diameters, lengths, and aspect ratios were 0.560 mum, 4.53 mum, and 8.62, respectively. Although whisker lengths were less than half those of the bulk material, nearly 30% of the whiskers were greater than 5 mum long.
引用
收藏
页码:315 / 319
页数:5
相关论文
共 50 条
  • [1] CHARACTERIZATION OF SILICON-CARBIDE WHISKERS
    KARASEK, KR
    BRADLEY, SA
    DONNER, JT
    YEH, HC
    SCHIENLE, JL
    FANG, HT
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1989, 72 (10) : 1907 - 1913
  • [2] CHARACTERIZATION OF RECENT SILICON-CARBIDE WHISKERS
    KARASEK, KR
    BRADLEY, SA
    DONNER, JT
    YEH, HC
    SCHIENLE, JL
    JOURNAL OF MATERIALS SCIENCE, 1991, 26 (01) : 103 - 111
  • [3] SILICON-CARBIDE WHISKERS
    BRAY, DJ
    AMERICAN CERAMIC SOCIETY BULLETIN, 1994, 73 (06): : 127 - 129
  • [4] SILICON-CARBIDE WHISKERS
    BRAY, DJ
    AMERICAN CERAMIC SOCIETY BULLETIN, 1995, 74 (06): : 152 - 153
  • [5] SILICON-CARBIDE WHISKERS
    BRAY, DJ
    AMERICAN CERAMIC SOCIETY BULLETIN, 1993, 72 (06): : 116 - 117
  • [6] SILICON-CARBIDE WHISKERS - CHARACTERIZATION AND AERODYNAMIC BEHAVIORS
    CHENG, YS
    POWELL, QH
    SMITH, SM
    JOHNSON, NF
    AMERICAN INDUSTRIAL HYGIENE ASSOCIATION JOURNAL, 1995, 56 (10): : 970 - 978
  • [7] A SUBCHRONIC INHALATION TOXICITY STUDY IN RATS EXPOSED TO SILICON-CARBIDE WHISKERS
    LAPIN, CA
    CRAIG, DK
    VALERIO, MG
    MCCANDLESS, JB
    BOGOROCH, R
    FUNDAMENTAL AND APPLIED TOXICOLOGY, 1991, 16 (01): : 128 - 146
  • [8] DEFECTS IN SILICON-CARBIDE WHISKERS
    NUTT, SR
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1984, 67 (06) : 428 - 431
  • [9] DEFECTS IN SILICON-CARBIDE WHISKERS
    NUTT, SR
    BREWER, W
    JOURNAL OF METALS, 1983, 35 (08): : A1 - A1
  • [10] TOXICITY OF SILICON-CARBIDE WHISKERS
    BIRCHALL, JD
    STANLEY, DR
    MOCKFORD, MJ
    PIGOTT, GH
    PINTO, PJ
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1988, 7 (04) : 350 - 352