COMPARISON OF THE MARGINAL AND AXIAL WALL INTEGRITY OF INVIVO AND INVITRO MADE ADHESIVE CLASS-V RESTORATIONS

被引:14
作者
ABDALLA, AI [1 ]
DAVIDSON, CL [1 ]
机构
[1] ACAD CTR DENT AMSTERDAM,DEPT DENT MAT SCI,LOUWESWEG 1,1066 EA AMSTERDAM,NETHERLANDS
关键词
D O I
10.1111/j.1365-2842.1993.tb01608.x
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
For several different procedures and material combinations adhesive Class V composite restorations were made under clinical and under laboratory conditions. Marginal discrepancy and gap formation at the floor of the cavity was recorded by way of SEM on replicas. Only weak correlation could be demonstrated between results obtained from in vivo and in vitro placed restorations. In general the hydrophobic resinous bonding systems performed better under laboratory conditions while the hydrophillic glass ionomer lining led to a better marginal integrity under clinical circumstances.