CLEAVAGE-LIKE FRACTURE ALONG SLIP PLANES IN FE-18CR-3NI-13MN-0.37N AUSTENITIC STAINLESS-STEEL AT LIQUID-HELIUM TEMPERATURE

被引:75
|
作者
TOBLER, RL [1 ]
MEYN, D [1 ]
机构
[1] USN,RES LAB,WASHINGTON,DC 20375
关键词
D O I
10.1007/BF02674040
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
引用
收藏
页码:1626 / 1631
页数:6
相关论文
共 6 条
  • [1] CLEAVAGE-LIKE FRACTURE ALONG SLIP PLANES IN Fe-18Cr-3Ni-13Mn-0. 37N AUSTENITIC STAINLESS STEEL AT LIQUID HELIUM TEMPERATURE.
    Tobler, R.L.
    Meyn, D.
    Metallurgical transactions. A, Physical metallurgy and materials science, 1988, 19 A (06): : 1626 - 1631
  • [2] CLEAVAGE-LIKE FRACTURE AT LOW-TEMPERATURES IN AN 18MN-18CR-0.5N AUSTENITIC STEEL
    TOMOTA, Y
    ENDO, S
    ISIJ INTERNATIONAL, 1990, 30 (08) : 656 - 662
  • [3] Fracture Behavior of thick-section weldment in Fe-12Cr-12Ni10Mn-0.24N stainless steel at liquid helium temperature
    Shindo, Y
    Horiguchi, K
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2004, 35A (12): : 3797 - 3802
  • [4] Fracture behavior of thick-section weldment in Fe-12Cr-12Ni-10Mn-0.24N stainless steel at liquid helium temperature
    Y. Shindo
    K. Horiguchi
    Metallurgical and Materials Transactions A, 2004, 35 : 3797 - 3802
  • [5] A Study on the Liquid Helium Temperature Tensile Property of Fe-21Cr-15Ni-5Mn-2Mo Austenitic Stainless Steel after Solution Treatment
    Zhang, Mengxing
    Wang, Changjun
    Ma, Dangshen
    Liu, Yu
    Wang, Weijun
    Liang, Jianxiong
    Fang, Chao
    Chu, Weihan
    Huang, Chuanjun
    MATERIALS, 2024, 17 (18)
  • [6] Strain-Induced Martensite Formation and Mechanical Properties of Fe-19Cr-4Ni-3Mn-0.15N-0.15C Austenitic Stainless Steel at Cryogenic Temperature
    Alsultan, Saba
    Quitzke, Caroline
    Cheng, Zhaoyang
    Krueger, Lutz
    Volkova, Olena
    Wendler, Marco
    STEEL RESEARCH INTERNATIONAL, 2021, 92 (06)