INITIAL-STAGES OF COPPER CORROSION IN HUMID AIR CONTAINING SO2 AND NO2

被引:59
作者
ERIKSSON, P
JOHANSSON, LG
STRANDBERG, H
机构
[1] CHALMERS UNIV TECHNOL,DEPT INORGAN CHEM,S-41296 GOTHENBURG,SWEDEN
[2] GOTHENBURG UNIV,S-41296 GOTHENBURG,SWEDEN
关键词
D O I
10.1149/1.2056109
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
We report on the reaction of SO2 and NO2 in sub-ppm concentrations in humid air with a copper surface. The deposition of SO2 was studied in a time-resolved manner and the formation of HNO2 was measured. Corrosion products were analyzed using XRD, FTIR, FTIRAS, and ion chromatography. S(IV)-O species on the copper surface was analyzed quantitatively using a sensitivity of 10-(11) mol. Corrosion rates and corrosion products are reported. The corrosion of copper in humid SO2-polluted air is accelerated strongly by the presence of NO2.
引用
收藏
页码:53 / 59
页数:7
相关论文
共 27 条
[1]   INTERACTION OF SO2 WITH COPPER AND COPPER-OXIDE SURFACES [J].
BAXTER, JP ;
GRUNZE, M ;
KONG, CW .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1988, 6 (03) :1123-1127
[2]  
ERICSSON R, 1977, WERKST KORROS, V28, P154
[3]   THE FORMATION OF SULFURIC-ACID, NITROGEN MONOXIDE, AND NITROUS-ACID ON GOLD IN AIR CONTAINING SUB-PPM CONCENTRATIONS OF SO2 AND NO2 [J].
ERIKSSON, P ;
JOHANSSON, LG .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1991, 138 (05) :1227-1233
[4]  
ERIKSSON P, 1991, UNPUB
[5]   A SODIUM-CARBONATE COATED DENUDER FOR DETERMINATION OF NITROUS-ACID IN THE ATMOSPHERE [J].
FERM, M ;
SJODIN, A .
ATMOSPHERIC ENVIRONMENT, 1985, 19 (06) :979-983
[6]  
GRADEL TE, 1987, CORROS SCI, V27, P721
[7]  
GRADEL TE, 1987, CORROS SCI, V27, P639
[8]  
GRADEL TE, 1987, CORROS SCI, V27, P741
[9]   OXIDATION OF SULFUR-DIOXIDE IN AQUEOUS SYSTEMS WITH PARTICULAR REFERENCE TO ATMOSPHERE [J].
HEGG, DA ;
HOBBS, PV .
ATMOSPHERIC ENVIRONMENT, 1978, 12 (1-3) :241-253
[10]  
HEIMLER B, 1971, 6TH P SCAN CORR C GO