MECHANICAL-PROPERTIES OF STRONTIUM FERRITES WITH DUPLEX STRUCTURE

被引:4
作者
WATARI, T [1 ]
HYAKUTAKE, H [1 ]
TORIKAI, T [1 ]
MATSUDA, O [1 ]
ENDO, M [1 ]
MOTONE, T [1 ]
机构
[1] KYUSYU SUMITOKU ELECTR CO LTD,OHMACHI,SAGA 84921,JAPAN
关键词
D O I
10.1016/0272-8842(95)95877-K
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The microstructures and the mechanical properties of the strontium ferrites (Sr-ferrites) with duplex structure were examined. As-received Sr-ferrites had a homogeneous microstructure and their average grain size was 1.58 mu m. Some grains increased up to 106 mu m and 228 mu m in size after annealing at 1250 degrees C for 1 h and 6 h, respectively. The volume fractions of the large grains were 4% after 1 h-annealing and 45% after 6 h-annealing. According to the microstructural evolution, the bending strength decreased from 148 MPa (as-received) to 140 MPa (3 h-annealing) and 93 MPa (6 h-annealing), but the fracture toughness increased from 2.14 MPa . m(1/2) (as-received) to 2.20 MPa . m(1/2) (3 h-annealing) and 2.36 MPa. m(1/2) (6 h-annealing). These results indicated that the large grains in the duplex structure acted as both fracture origins and reinforcements. The Weibull modulus of materials was improved from 7 (as-received materials) to 17 (material after 3 h-annealing) and 9.5 (material after 6 h-annealing).
引用
收藏
页码:89 / 95
页数:7
相关论文
共 23 条
[1]   MICROSTRUCTURAL DESIGN OF TOUGHENED CERAMICS [J].
BECHER, PF .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1991, 74 (02) :255-269
[2]   INSITU ALUMINA ALUMINATE PLATELET COMPOSITES [J].
CHEN, PL ;
CHEN, IW .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1992, 75 (09) :2610-2612
[3]  
CLAASSEN T, 1992, J EUR CERAM SOC, V10, P263, DOI 10.1016/0955-2219(92)90040-K
[4]  
CLAUSSEN N, 1990, STRUCTURAL CERAMICS, P1
[5]  
HAMAMURA A, 1973, SUMITOMO TOKUSYU KIN, V1, P37
[6]   UNIQUE OPPORTUNITIES FOR MICROSTRUCTURAL ENGINEERING WITH DUPLEX AND LAMINAR CERAMIC COMPOSITES [J].
HARMER, MP ;
CHAN, HM ;
MILLER, GA .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1992, 75 (07) :1715-1728
[7]   FRACTURE OF ISOTROPIC AND TEXTURED BA HEXAFERRITE [J].
IWASA, M ;
LIANG, EC ;
BRADT, RC ;
NAKAMURA, Y .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (07) :390-393
[8]  
KINGERY WD, 1976, INTRO CERAMICS, P461
[9]   PRESSURELESS SINTERING OF SIC-WHISKER-REINFORCED AL2O3 COMPOSITES .1. EFFECT OF MATRIX POWDER SURFACE-AREA [J].
LEE, HW ;
SACKS, MD .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (07) :1884-1893
[10]   TOPOTACTICAL REACTIONS WITH FERRIMAGNETIC OXIDES HAVING HEXAGONAL CRYSTAL STRUCTURES .1. [J].
LOTGERING, FK .
JOURNAL OF INORGANIC & NUCLEAR CHEMISTRY, 1959, 9 (02) :113-+