THE RELATIONSHIP BETWEEN MICROSTRUCTURE AND MODE OF FRACTURE IN POLYHYDROXYBUTYRATE

被引:219
作者
BARHAM, PJ
KELLER, A
机构
关键词
D O I
10.1002/polb.1986.180240108
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
引用
收藏
页码:69 / 77
页数:9
相关论文
共 12 条
[1]   PROBLEM OF THERMAL-EXPANSION IN POLYETHYLENE SPHERULITES [J].
BARHAM, PJ ;
KELLER, A .
JOURNAL OF MATERIALS SCIENCE, 1977, 12 (11) :2141-2148
[2]   NUCLEATION BEHAVIOR OF POLY-3-HYDROXY-BUTYRATE [J].
BARHAM, PJ .
JOURNAL OF MATERIALS SCIENCE, 1984, 19 (12) :3826-3834
[3]   CRYSTALLIZATION AND MORPHOLOGY OF A BACTERIAL THERMOPLASTIC - POLY-3-HYDROXYBUTYRATE [J].
BARHAM, PJ ;
KELLER, A ;
OTUN, EL ;
HOLMES, PA .
JOURNAL OF MATERIALS SCIENCE, 1984, 19 (09) :2781-2794
[4]   EFFECT OF POLYMERIZATION CONDITIONS AND CRYSTALLINITY ON MECHANICAL-PROPERTIES AND FRACTURE OF SPHERULITIC NYLON-6 [J].
BESSELL, TJ ;
HULL, D ;
SHORTALL, JB .
JOURNAL OF MATERIALS SCIENCE, 1975, 10 (07) :1127-1136
[5]  
FRIEDRICH K, 1983, ADV POLYM SCI, V52-3, P225
[6]   THE THERMAL-DEGRADATION OF POLY(-(D)-BETA-HYDROXYBUTYRIC ACID) .1. IDENTIFICATION AND QUANTITATIVE-ANALYSIS OF PRODUCTS [J].
GRASSIE, N ;
MURRAY, EJ ;
HOLMES, PA .
POLYMER DEGRADATION AND STABILITY, 1984, 6 (01) :47-61
[7]   THE THERMAL-DEGRADATION OF POLY(-(D)-BETA-HYDROXYBUTYRIC ACID) .2. CHANGES IN MOLECULAR-WEIGHT [J].
GRASSIE, N ;
MURRAY, EJ ;
HOLMES, PA .
POLYMER DEGRADATION AND STABILITY, 1984, 6 (02) :95-103
[8]   REGIME-III CRYSTALLIZATION IN MELT-CRYSTALLIZED POLYMERS - THE VARIABLE CLUSTER MODEL OF CHAIN FOLDING [J].
HOFFMAN, JD .
POLYMER, 1983, 24 (01) :3-26
[9]  
HOWELLS ER, 1982, CHEM IND-LONDON, P508
[10]   SOME STUDIES OF DEFORMATION PROCESSES IN FULLY-SPHERULITIC POLYPROPYLENE [J].
WAY, JL ;
ATKINSON, JR .
JOURNAL OF MATERIALS SCIENCE, 1971, 6 (02) :102-&