TENSILE CREEP AND CREEP-RUPTURE BEHAVIOR OF MONOLITHIC AND SIC-WHISKER-REINFORCED SILICON-NITRIDE CERAMICS

被引:56
作者
OHJI, T
YAMAUCHI, Y
机构
[1] National Industrial Research Institute of Nagoya
关键词
D O I
10.1111/j.1151-2916.1993.tb06615.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The tensile creep and creep rupture behavior of silicon nitride was investigated at 1200-degrees to 1350-degrees-C using hot-pressed materials with and without SiC whiskers. Stable steady-state creep was observed under low applied stresses at 1200-degrees-C. Accelerated creep regimes, which were absent below 1300-degrees-C, were identified above that temperature. The appearance of accelerated creep at the higher temperatures is attributable to formation of microcracks throughout a specimen. The whisker-reinforced material exhibited better creep resistance than the monolith at 1200-degrees-C; however, the superiority disappeared above 1300-degrees-C. Considerably high values, 3 to 5, were obtained for the creep exponent in the overall temperature range. The exponent tended to decrease with decreasing applied stress at 1200-degrees-C. The primary creep mechanism was considered cavitation-enhanced creep. Specimen lifetimes followed the Monkman-Grant relationship except for fractures with large accelerated creep regimes. The creep rupture behavior is discussed in association with cavity formation and crack coalescence.
引用
收藏
页码:3105 / 3112
页数:8
相关论文
共 42 条
[1]   CREEP AND STRAIN RECOVERY IN HOT-PRESSED SILICON-NITRIDE [J].
ARONS, RM ;
TIEN, JK .
JOURNAL OF MATERIALS SCIENCE, 1980, 15 (08) :2046-2058
[2]   TECHNIQUE FOR TENSILE CREEP TESTING OF CERAMICS [J].
CARROLL, DF ;
WIEDERHORN, SM ;
ROBERTS, DE .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1989, 72 (09) :1610-1614
[3]   EFFECT OF CREEP DAMAGE ON THE TENSILE CREEP-BEHAVIOR OF A SILICONIZED SILICON-CARBIDE [J].
CARROLL, DF ;
TRESSLER, RE .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1989, 72 (01) :49-53
[4]   CAVITY NUCLEATION AT GRAIN-BOUNDARY LEDGES [J].
CHAN, KS ;
PAGE, RA ;
LANKFORD, J .
ACTA METALLURGICA, 1986, 34 (12) :2361-2370
[5]  
CHOKSHI AH, 1985, J AM CERAM SOC, V68
[6]  
DEBSCHUTZ KD, 1991, 93RD ANN M AM CER SO
[7]  
DRUCKER DC, 1965, HIGH STRENGTH MATERI, P795
[8]   CREEP DEFORMATION DUE TO A VISCOUS GRAIN-BOUNDARY PHASE [J].
DRYDEN, JR ;
KUCEROVSKY, D ;
WILKINSON, DS ;
WATT, DF .
ACTA METALLURGICA, 1989, 37 (07) :2007-2015
[9]   MICROSTRUCTURAL STUDIES ON SILICON NITRIDE [J].
EVANS, AG ;
SHARP, JV .
JOURNAL OF MATERIALS SCIENCE, 1971, 6 (10) :1292-&
[10]   HIGH-TEMPERATURE FAILURE MECHANISMS IN CERAMICS [J].
EVANS, AG ;
RANA, A .
ACTA METALLURGICA, 1980, 28 (02) :129-141