HOT FILAMENT ACTIVATED CHEMICAL VAPOR-DEPOSITION OF BORON-NITRIDE

被引:22
|
作者
RYE, RR
机构
[1] Sandia National Laboratories, Albuquerque
关键词
D O I
10.1116/1.577583
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Using a hot filament (almost-equal-to 1400-degrees-C) to activate borazine (B3N3H6) molecules for subsequent reaction with a direct line-of-sight substrate, transparent boron nitride films as thick as 25 000 angstrom have been grown for substrate temperatures as low as 100-degrees-C. The minimum temperature is determined by radiative heating from the adjacent hot filament. The low temperature BN films show no indication of crystallinity with x-ray diffraction (XRD), but the opaque BN deposit produced on the hot filament is identified by XRD as polycrystalline h-BN. X-ray photoelectron spectra (XPS) show the films to have a B:N ratio (within experimental error) of 1:1 with no other XPS detectable impurities above the 0.5% level. Both Raman and infrared (IR) spectroscopy are characteristic of h-BN with small amounts of hydrogen detected as N-H and B-H bands in the IR spectrum. The important feature of this method is the separation and localization of the thermal activation step at the hot filament from the surface reaction and film growth steps at the substrate surface. This allows both higher temperature thermal activation and lower temperature film growth.
引用
收藏
页码:1099 / 1103
页数:5
相关论文
共 50 条
  • [41] EVIDENCE OF A SHALLOW JUNCTION FORMATION FROM PLASMA-ENHANCED CHEMICAL-VAPOR-DEPOSITION OF BORON-NITRIDE AND SILICON BORON-NITRIDE
    NGUYEN, T
    VANNGUYEN, S
    DOBUZINSKY, DM
    APPLIED PHYSICS LETTERS, 1993, 63 (15) : 2103 - 2105
  • [42] PLASMA-ASSISTED CHEMICAL-VAPOR-DEPOSITION AND CHARACTERIZATION OF BORON-NITRIDE FILMS
    NGUYEN, SV
    NGUYEN, T
    TREICHEL, H
    SPINDLER, O
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1994, 141 (06) : 1633 - 1638
  • [43] Diamond synthesis on silicon nitride by the hot filament chemical vapor deposition technique
    Universita di Roma `Tor Vergata', Roma, Italy
    J Ceram Soc Jpn, 1240 (1167-1171):
  • [44] Diamond synthesis on silicon nitride by the hot filament chemical vapor deposition technique
    Polini, R
    Mattei, G
    Marucci, A
    Traversa, E
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1998, 106 (12) : 1167 - 1171
  • [45] PLASMA-ENHANCED CHEMICAL-VAPOR-DEPOSITION OF BORON-NITRIDE ONTO INP
    BATH, A
    BAEHR, O
    BARRADA, M
    LEPLEY, B
    VANDERPUT, PJ
    SCHOONMAN, J
    THIN SOLID FILMS, 1994, 241 (1-2) : 278 - 281
  • [46] PROPERTIES OF BORON-NITRIDE COATING FILMS PREPARED BY THE ION-BEAM AND VAPOR-DEPOSITION METHOD (IVD)
    ANDOH, Y
    OGATA, K
    SUZUKI, Y
    KAMIJO, E
    SATOU, M
    FUJIMOTO, F
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 1987, 19-20 : 787 - 790
  • [47] CHEMICAL VAPOR-DEPOSITION OF SILICON-NITRIDE
    BUHLER, J
    FITZER, E
    KEHRE, D
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1977, 124 (08) : C299 - C299
  • [48] CHEMICAL VAPOR-DEPOSITION OF SILICON-NITRIDE
    GEBHARDT, JJ
    TANZILLI, RA
    HARRIS, TA
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1976, 123 (10) : 1578 - 1582
  • [49] CHEMICAL VAPOR-DEPOSITION OF TANTALUM NITRIDE FILMS
    TAKAHASHI, T
    ITOH, H
    OZEKI, S
    JOURNAL OF THE LESS-COMMON METALS, 1977, 52 (01): : 29 - 36
  • [50] KINETICS OF CHEMICAL VAPOR-DEPOSITION OF TITANIUM NITRIDE
    NAKANISHI, N
    MORI, S
    KATO, E
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1990, 137 (01) : 322 - 328