EFFECT OF INCLUSION CONTENT ON THE CREEP-RUPTURE PROPERTIES OF TYPE 17CR-8NI-2MO WELD METALS

被引:6
作者
SENIOR, BA
机构
[1] CEGB, United Kingdom
关键词
Stainless Steel--Welding - Welding--Electrodes;
D O I
10.1007/BF01111905
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
It has been known for some time that austenitic weldments exhibit low and variable creep rupture properties, but many of the factors controlling these properties are not well understood. In this investigation, two welds (Type 316) with similar compositions and fabricated using the same welding parameters, but with different electrode coatings, have been examined after creep testing. The results indicate that the inclusion and silicon content of type 316 welds can strongly influence their creep rupture properties, a high inclusion density being associated with poor creep rupture properties, and a low silicon content with a higher creep rate. This has been explained with reference to the micromechanism of creep failure operating in these welds.
引用
收藏
页码:2479 / 2484
页数:6
相关论文
共 26 条
  • [1] FINITE-ELEMENT ANALYSIS OF VOID GROWTH NEAR A BLUNTING CRACK TIP
    ARAVAS, N
    MCMEEKING, RM
    [J]. JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 1985, 33 (01) : 25 - 49
  • [2] MICROSTRUCTURAL ORIGIN OF THE SKELETAL FERRITE MORPHOLOGY OF AUSTENITIC STAINLESS-STEEL WELDS
    BROOKS, JA
    WILLIAMS, JC
    THOMPSON, AW
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1983, 14 (07): : 1271 - 1281
  • [3] STEM ANALYSIS OF PRIMARY AUSTENITE SOLIDIFIED STAINLESS-STEEL WELDS
    BROOKS, JA
    WILLIAMS, JC
    THOMPSON, AW
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1983, 14 (01): : 23 - 31
  • [4] CHUNG FH, 1974, ADV XRAY ANAL, V17
  • [5] CIESLAK MJ, 1982, WELD J, V61, P1
  • [6] DEIGHTON M, 1970, J IRON STEEL I, V208, P1012
  • [7] DELONG WT, 1974, WELD J, V53, P273
  • [8] Hammar O., 1979, MET SOC, P401
  • [9] HARRIES DR, 1981, 1980 P INT C MECH BE, P1
  • [10] HORSFIELD AM, 1983, STAINLESS STEEL IND, V11, P9