Thermoelectric properties of cold pressed samples of semiconductor (Bi1-XSbX)(2)Te-3 solid solutions

被引:3
作者
Martynova, K. V. [1 ]
Rogacheva, E. I. [1 ]
机构
[1] Natl Tech Univ, Kharkiv Polytech Inst, 2 Kyrpychova Str, UA-61002 Kharkov, Ukraine
来源
FUNCTIONAL MATERIALS | 2018年 / 25卷 / 01期
关键词
(Bi1-XSbX)(2)Te-3 solid solutions; cold pressing; annealing; Seebeck coefficient; electrical conductivity; thermal conductivity; figure of merit;
D O I
10.15407/fm25.01.54
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The composition dependences of thermoelectric (TE) properties of (Bi1-XSbX)(2)Te-3 solid solutions (0 < x < 1) produced by cold pressing and subsequent annealing were investigated at room temperature. Samples were prepared from cast polycrystals, obtained by the cooling of melt down to room temperature in evacuated quartz ampoules and subsequent annealing. It was established that cast samples exhibited p-type conductivity in the entire composition range, and an increase in the Sb2Te3 content led to the growth of electrical conductivity and drop of the Seebeck coefficient. The change of the conductivity type from positive to negative in the composition range x = 0 - 0.6 took place after cold pressing and composition dependencies of the properties became more complex. The maximum figure of merit value (Z(max) = (3.1 +/- 0.4).10(-3) K-1) that was achieved in cold-pressed annealed samples at x = 0.8 was comparable to the values of Z for single crystals of undoped (Bi1-XSbX)(2)Te-3 solid solutions and for polycrystalline samples produced by other methods. It follows from the data obtained that the proposed method of preparing the samples of (Bi1-XSbX)(2)Te-3 solid solutions by cold pressing and subsequent annealing may appear to be useful in thermoelectric devices.
引用
收藏
页码:54 / 60
页数:7
相关论文
共 37 条
  • [1] Abrikosov N.Kh, 2013, MONOGRAPHS SEMICONDU, P252
  • [2] Abrikosov N.Kh, 1965, IAN SSSR NEORG MATER, V1, P503
  • [3] THERMOELECTRIC PROPERTIES OF FINE-GRAINED (75-PERCENT-SB2TE3-25-PERCENT-BI2TE3) P-TYPE AND (90-PERCENT-BI2TE3-5-PERCENT-SB2TE3-5-PERCENT-SB2SE3) N-TYPE ALLOYS
    AMIN, FAA
    ALGHAFFARI, ASS
    ISSA, MAA
    HASSIB, AM
    [J]. JOURNAL OF MATERIALS SCIENCE, 1992, 27 (05) : 1250 - 1254
  • [4] Belov J.M., 1998, P ICT 98 17 INT C TH, P247
  • [5] Bulat LP, 2012, DELIVERY OF NANOPARTICLES, P453
  • [6] THERMOELECTRIC PROPERTIES OF BI2TE3-SB2TE3 ALLOYS
    CHAMPNESS, CH
    CHIANG, PT
    PAREKH, P
    [J]. CANADIAN JOURNAL OF PHYSICS, 1965, 43 (04) : 653 - +
  • [7] Thermoelectric properties of p-type Te-doped (Bi,Sb)2Te3 alloys by mechanical alloying and plasma activated sintering
    Fan, Xi'an
    Yang, Junyou
    Zhu, Wen
    Bao, Siqian
    Duan, Xingkai
    Zhang, Qinqin
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 448 (1-2) : 308 - 312
  • [8] Goldsmid HJ, 2016, SPRINGER SER MATER S, V121, P1, DOI 10.1007/978-3-662-49256-7
  • [9] Effects of excess Te on the thermoelectric properties of p-type 25% Bi2Te3-75% Sb2Te3 single crystal and hot-pressed sinter
    Hwang, CW
    Hyun, DB
    Ha, HP
    Oh, TS
    [J]. JOURNAL OF MATERIALS SCIENCE, 2001, 36 (13) : 3291 - 3297
  • [10] Ivanova L.D., 2011, INORG MATER, V47, P521