FRACTURE AND SUBCRITICAL CRACK-GROWTH IN SODA-LIME GLASS UNDER COMBINED MODE-I AND MODE-II LOADING

被引:3
作者
YODA, M [1 ]
YOSHIKAWA, Y [1 ]
ONO, K [1 ]
IDE, M [1 ]
机构
[1] SANKYO SEIKI MFG CO LTD,SUWA,NAGANO 393,JAPAN
关键词
D O I
10.1111/j.1151-2916.1995.tb08376.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Fracture and subcritical crack growth characteristics under combined modes I and II loading were studied using the compact tension shear specimens of soda-line glass. The maximum normal stress criterion gives a good agreement with the experimental mode I-mode II fracture toughness envelope for initially straight cracks and kinked cracks. Subcritical crack growth characteristics were determined under sustained modes I and II loading in water. The values of K-I and K-II were calculated approximately by replacing the subcritical kinked crack with an assumed straight crack (a) over bar, and the K-Imax value based on the maximum normal stress criterion was used to describe this subcritical kinked crack growth. The experimental results show that subcritical crack growth under pure mode I, pure mode II, and various combined modes I and II loading can be well described by the K-Imax value based on the approximate maximum normal stress criterion.
引用
收藏
页码:161 / 165
页数:5
相关论文
共 17 条
[1]  
Erdogan F., 1963, J BASIC ENG, V85, P519, DOI DOI 10.1115/1.3656897
[2]   PROOF TESTING OF CERAMIC MATERIALS - ANALYTICAL BASIS FOR FAILURE PREDICTION [J].
EVANS, AG ;
WIEDERHORN, SM .
INTERNATIONAL JOURNAL OF FRACTURE, 1974, 10 (03) :379-392
[3]   ENVIRONMENTALLY ENHANCED CRACK-GROWTH IN SODA-LIME GLASS [J].
FREIMAN, SW ;
WHITE, GS ;
FULLER, ER .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1985, 68 (03) :108-112
[4]   MIXED-MODE FRACTURE IN SODA-LIME GLASS [J].
FREIMAN, SW ;
GONZALEZ, AC ;
MECHOLSKY, JJ .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1979, 62 (3-4) :206-208
[5]   MIXED-MODE CRACK-GROWTH PREDICTIONS [J].
GDOUTOS, EE .
ENGINEERING FRACTURE MECHANICS, 1987, 28 (02) :211-221
[6]   MIXED-MODE FRACTURE IN SODA-LIME GLASS USING INDENTATION FLAWS [J].
GLAESEMANN, GS ;
RITTER, JE ;
JAKUS, K .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1987, 70 (09) :630-636
[7]  
Hussian M.A., 1974, ASTM STP, V560, P2
[8]   MECHANISMS OF FAILURE FROM SURFACE FLAWS IN MIXED-MODE LOADING [J].
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1984, 67 (02) :110-116
[9]   STRAIN ENERGY DENSITY FACTOR APPLIED TO MIXED MODE CRACK PROBLEMS [J].
SIH, GC .
INTERNATIONAL JOURNAL OF FRACTURE, 1974, 10 (03) :305-321
[10]   SUBCRITICAL CRACK-GROWTH IN SODA-LIME GLASS IN COMBINED MODE-I AND MODE-II LOADING [J].
SINGH, D ;
SHETTY, DK .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (12) :3597-3606