CORROSION FATIGUE CHARACTERISTICS OF 304-STAINLESS STEEL AND AE-ANALYSIS DURING THE PROCESS (MONITORING OF CRACKING AND AE-SOURCES)

被引:3
作者
YUYAMA, S [1 ]
HISAMATSU, Y [1 ]
KISHI, T [1 ]
机构
[1] UNIV TOKYO, FAC ENGN, DEPT MET & MAT SCI, TOKYO 113, JAPAN
关键词
All Open Access; Bronze;
D O I
10.2320/jinstmet1952.46.1_85
中图分类号
学科分类号
摘要
Stainless steel
引用
收藏
页码:85 / 93
页数:9
相关论文
共 8 条
[1]  
DOIG P, 1978, METALL TRANS A, V9, P357, DOI 10.1007/BF02646385
[2]  
Hartbower C. E., 1972, ASTM STP, V505, P187
[3]   ACOUSTIC-EMISSION TRANSDUCER AND ITS ABSOLUTE CALIBRATION [J].
HATANO, H ;
MORI, E .
JOURNAL OF THE ACOUSTICAL SOCIETY OF AMERICA, 1976, 59 (02) :344-349
[4]  
KOMURA I, 1981, ADV AE, P195
[5]  
KUSANAGI H, 1980, 5TH P INT AC EM S TO, P125
[6]  
MONDEN Y, 1978, 4TH P INT AE S TOK
[7]  
Ohira T, 1980, 5TH P INT AE S, P137
[8]   APPLICATION OF ACOUSTIC-EMISSION TECHNIQUE TO STUDY OF STRESS-CORROSION CRACKING IN DISTINGUISHING BETWEEN ACTIVE PATH CORROSION AND HYDROGEN EMBRITTLEMENT [J].
OKADA, H ;
YUKAWA, KI ;
TAMURA, H .
CORROSION, 1974, 30 (07) :253-255