TENSILE PROPERTIES INFLUENCING VARIABLES IN EUTECTIC AL-SI CASTING ALLOYS

被引:13
作者
HAFIZ, MF [1 ]
KOBAYASHI, T [1 ]
机构
[1] TOYOHASHI UNIV TECHNOL,DEPT PROD SYST ENGN,TOYOHASHI,AICHI 441,JAPAN
来源
SCRIPTA METALLURGICA ET MATERIALIA | 1994年 / 31卷 / 06期
关键词
Aluminum castings alloy - Brittle fracture - Plastic deformation - Solidification cooling - Tensile properties;
D O I
10.1016/0956-716X(94)90213-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
[No abstract available]
引用
收藏
页码:701 / 705
页数:5
相关论文
共 9 条
[1]   DAMAGE INITIATION IN METAL MATRIX COMPOSITES [J].
BRECHET, Y ;
EMBURY, JD ;
TAO, S ;
LUO, L .
ACTA METALLURGICA ET MATERIALIA, 1991, 39 (08) :1781-1786
[2]  
Closset B., 1982, AFS T, V90, P453
[3]  
DAVAMI P, 1979, BRIT FOUNDRYMAN, V72, P4
[4]   MICROSTRUCTURE AND MECHANICAL-PROPERTIES OF MODIFIED AND NON-MODIFIED STIR-CAST AL-SI HYPOEUTECTIC ALLOYS [J].
FATHALLA, N ;
SECORDEL, P ;
SUERY, M .
JOURNAL OF MATERIALS SCIENCE, 1988, 23 (07) :2419-2423
[5]  
Hafiz M. F., 1994, Journal of Japan Institute of Light Metals, V44, P28, DOI 10.2464/jilm.44.28
[6]   A STUDY ON THE MICROSTRUCTURE-FRACTURE BEHAVIOR RELATIONS IN AL-SI CASTING ALLOYS [J].
HAFIZ, MF ;
KOBAYASHI, T .
SCRIPTA METALLURGICA ET MATERIALIA, 1994, 30 (04) :475-480
[7]  
HAFIZ MF, 1990, Z METALLKD, V81, P70
[8]  
HAQUE MM, 1983, MET FORUM, V6, P54
[9]  
HELLAWELL A, 1973, PROGR MATER SCI, P15