共 50 条
- [31] Cleavage fracture toughness of tempered martensitic Ni-Cr-Mo low alloy steel with different martensite fraction MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 534 : 75 - 82
- [33] EFFECT OF HYDROGEN ATMOSPHERE ON CRACK INITIATION IN HEAT-TREATED 3.5NI-CR-MO-V STEEL METALS TECHNOLOGY, 1982, 9 (MAR-): : 143 - 148
- [35] Effect of nickel additions on microstructure evolution and mechanical properties of low-alloy Cr-Mo cast steel INTERNATIONAL SEMINAR ON METALLURGY AND MATERIALS, 2019, 541
- [36] Effect of Tempering on the Ductile-to-Brittle Transitional Behavior of Ni-Cr-Mo Low-Alloy Steel Experimental Mechanics, 2020, 60 : 1167 - 1172
- [38] EFFECT OF HEAT-TREATMENT ON FRACTURE-TOUGHNESS OF 0.85-PERCENT-C-3-PERCENT-CR ROLL STEEL TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1988, 74 (10): : 2017 - 2024
- [39] Effect of tempering heat treatment on the microstructure and impact toughness of a Ni-Cr-Mo-V steel weld metal MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 850
- [40] Effect of Indirect Transformation of Retained Austenite During Tempering on the Charpy Impact Toughness of a Low-Alloy Cr–Mo–V Steel Acta Metallurgica Sinica (English Letters), 2020, 33 : 1346 - 1358