SPECTROSCOPIC AND SELECTED MECHANICAL-PROPERTIES OF DIAMOND-LIKE CARBON-FILMS SYNTHESIZED BY BROAD-BEAM ION DEPOSITION FROM METHANE

被引:19
作者
COOPER, CV
BEETZ, CP
BUCHHOLTZ, BW
WILBUR, PJ
WEI, R
机构
[1] ADV TECHNOL MAT, DANBURY, CT 06810 USA
[2] COLORADO STATE UNIV, FT COLLINS, CO 80523 USA
关键词
D O I
10.1016/0925-9635(94)90219-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Broad-beam ion deposition was employed to decompose methane for the synthesis of diamond-like-carbon (DLC or a-C: H) films, deposited to two thicknesses of approximately 1 and 5 mum onto AISI M50 substrates in the presence or absence of a submicrometer intermediate layer of either amorphous Si:C:H or elemental Si. During deposition from CH4 the current density supplied to the ion gun was maintained at a constant 2.5 mA cm-2, while the accelerating potential was varied over the range 250-700 eV. The resulting microstructures, characterized using scanning electron microscopy and stylus-type profilometry, revealed ultrasmooth and essentially featureless surfaces for all films. Raman spectroscopy produced spectra which could be deconvoluted most effectively by the superposition of peaks positioned at three wavenumbers, predominated by the peak ascribable to sp2-hybridized bonding; it was, however, unable to differentiate from among the films deposited at various ion-beam energies. Fourier-transform IR (FTIR) reflectivity revealed that the ratio of sp3 to sp2 carbon-bonded hydrogen in the films was approximately 3.5; FTIR results exhibited a modest trend toward decreasing sp-3 to sp2 ratio for films deposited with increasing ion-beam energy. Nanoindentation properties of hardness and elastic modulus were found to be essentially insensitive to ion accelerating energy; however, adherence between the film and mechanically polished M50 substrate as measured by the scratch technique displayed a modest dependence on accelerating energy, with a maximum critical force occurring for films deposited at the highest energy investigated, 677 eV. Conversely, an inverse relationship between friction coefficient and ion deposition energy emerged, with coefficients ranging between 0.105 and 0.153. The film grown to a thickness of approximately 5 mum exhibited decidedly inferior adherence to the M50 substrate than those grown to a thickness of approximately 1 mum. Deposition at an energy of 260 eV onto the elemental Si intermediate layer or deposition directly onto the M50 substrate in the absence of an intermediate layer failed to produce adherent films, spalling spontaneously either immediately or within days following deposition.
引用
收藏
页码:534 / 541
页数:8
相关论文
共 50 条
[1]   LOW-PRESSURE, METASTABLE GROWTH OF DIAMOND AND DIAMONDLIKE PHASES [J].
ANGUS, JC ;
HAYMAN, CC .
SCIENCE, 1988, 241 (4868) :913-921
[2]   THE EFFECT OF THE CONDITION OF THE SCRATCH DIAMOND ON MEASURED CRITICAL LOADS [J].
ARNELL, RD ;
EFEOGLU, I .
VACUUM, 1993, 44 (08) :805-807
[3]   ULTRALOW-LOAD INDENTATION HARDNESS AND MODULUS OF DIAMOND FILMS DEPOSITED BY HOT-FILAMENT-ASSISTED CVD [J].
BEETZ, CP ;
COOPER, CV ;
PERRY, TA .
JOURNAL OF MATERIALS RESEARCH, 1990, 5 (11) :2555-2561
[4]   STRUCTURE AND PROPERTIES OF TRANSPARENT AND HARD CARBON-FILMS [J].
BEWILOGUA, K ;
DIETRICH, D ;
PAGEL, L ;
SCHURER, C ;
WEISSMANTEL, C .
SURFACE SCIENCE, 1979, 86 (JUL) :308-313
[5]   THE EFFECTS OF METHANE CONCENTRATION IN HYDROGEN ON THE MICROSTRUCTURE AND PROPERTIES OF DIAMOND FILMS GROWN BY HOT-FILAMENT CHEMICAL VAPOR-DEPOSITION [J].
COOPER, CV ;
BEETZ, CP .
SURFACE & COATINGS TECHNOLOGY, 1991, 47 (1-3) :375-387
[6]  
COOPER CV, IN PRESS SURF COAT T
[7]   THE OPTICAL AND MECHANICAL-PROPERTIES OF CARBON-FILMS GROWN USING A FAST ATOM BEAM SOURCE [J].
DEHBIALAOUI, A ;
MATTHEWS, A ;
FRANKS, J .
SURFACE & COATINGS TECHNOLOGY, 1991, 47 (1-3) :722-729
[8]   MECHANICAL AND THERMOPHYSICAL PROPERTIES OF DIAMOND-LIKE CARBON (DLC) FILMS WITH DIFFERENT SP(3)/SP(2) RATIOS [J].
DEMICHELIS, F ;
PIRRI, CF ;
TAGLIAFERRO, A ;
BENEDETTO, G ;
BOARINO, L ;
SPAGNOLO, R ;
DUNLOP, E ;
HAUPT, J ;
GISSLER, W .
DIAMOND AND RELATED MATERIALS, 1993, 2 (5-7) :890-892
[9]   HARD CARBON COATINGS WITH LOW OPTICAL-ABSORPTION [J].
DISCHLER, B ;
BUBENZER, A ;
KOIDL, P .
APPLIED PHYSICS LETTERS, 1983, 42 (08) :636-638
[10]   A method for interpreting the data from depth-sensing indentation instruments [J].
Doerner, M. F. ;
Nix, W. D. .
JOURNAL OF MATERIALS RESEARCH, 1986, 1 (04) :601-609