ROOM-TEMPERATURE EROSION BEHAVIOR OF 304, 316 AND 410 STAINLESS-STEELS

被引:33
|
作者
SINGH, T [1 ]
TIWARI, SN [1 ]
SUNDARARAJAN, G [1 ]
机构
[1] BANARAS HINDU UNIV,DEPT MET,VARANASI 221005,UTTAR PRADESH,INDIA
关键词
D O I
10.1016/0043-1648(91)90240-U
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The main purpose of this investigation is to compare the room temperature erosion behaviour of three stainless steels, namely 304, 316 and 410 SS. Towards this purpose, the erosion rates of all three stainless steels have been determined at three impact angles (30-degrees, 60-degrees, and 90-degrees) and at two impact velocities (98 and 129 m s-1) for each angle. The results indicate that while the erosion rates of 304 and 316 SS are comparable, that of 410 SS is lower by 15%-20%. The improved erosion resistance of 410 SS, in spite of its lower ductility and strain-hardening capacity as compared with 304 and 316 SS, appears to be related to the fact that the depth to which plastic deformation extends beneath the eroded surface (L) is significantly lower in 410 SS and also to the presence of a "soft zone" beneath the eroded surface.
引用
收藏
页码:77 / 100
页数:24
相关论文
共 50 条
  • [1] Room temperature erosion behaviour of 304, 316 and 410 stainless steels
    Singh, Trilok
    Tiwari, S.N.
    Sundararajan, G.
    1600, (145):
  • [2] ROOM-TEMPERATURE CREEP-BEHAVIOR OF STAINLESS-STEELS
    TENDO, M
    TAKESHITA, T
    NAKAZAWA, T
    KIMURA, H
    ABO, H
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1993, 79 (01): : 98 - 104
  • [3] THE EFFECTS OF H ON THE MECHANICAL-BEHAVIOR OF AUSTENITIC STAINLESS-STEELS AT ROOM-TEMPERATURE
    LONG, QY
    FAN, CG
    XING, ZS
    LI, YY
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1994, 25 (05): : 1015 - 1023
  • [4] RELATIONSHIP BETWEEN ROOM-TEMPERATURE CREEP-BEHAVIOR AND YIELD STRENGTH IN AUSTENITIC STAINLESS-STEELS
    TENDO, M
    TAKESHITA, T
    NAKAZAWA, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1994, 80 (02): : 149 - 154
  • [5] DEFORMATION-INDUCED MARTENSITIC CHARACTERISTICS IN 304-STAINLESS AND 316-STAINLESS STEELS DURING ROOM-TEMPERATURE ROLLING
    SHRINIVAS, V
    VARMA, SK
    MURR, LE
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1995, 26 (03): : 661 - 671
  • [6] EROSION AND EROSION CORROSION BEHAVIOR OF CHROMIZED ALUMINIZED STAINLESS-STEELS AT ROOM AND ELEVATED-TEMPERATURES
    LIU, YJ
    LEVY, AV
    SURFACE & COATINGS TECHNOLOGY, 1990, 43-4 (1-3): : 836 - 847
  • [7] HIGH-TEMPERATURE EROSION-CORROSION BEHAVIOR OF STAINLESS-STEELS
    ZHOU, JR
    BAHADUR, S
    JOURNAL OF METALS, 1988, 40 (11): : 37 - 38
  • [8] EFFECTS OF SOLUTE CARBON AND NITROGEN ON ROOM-TEMPERATURE CREEP OF AUSTENITIC STAINLESS-STEELS
    TENDO, M
    TAKESHITA, T
    NAKAZAWA, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1995, 59 (06) : 620 - 626
  • [9] COMPARISON OF DYNAMIC SOFTENING IN 301, 304, 316 AND 317 STAINLESS-STEELS
    RYAN, ND
    MCQUEEN, HJ
    HIGH TEMPERATURE TECHNOLOGY, 1990, 8 (03): : 185 - 200
  • [10] Solid particle erosion of AISI 304, 316 and 420 stainless steels
    Laguna-Camacho, J. R.
    Marquina-Chavez, A.
    Mendez-Mendez, J. V.
    Vite-Torres, M.
    Gallardo-Hernandez, E. A.
    WEAR, 2013, 301 (1-2) : 398 - 405