摘要
Low concentrations of about 6. 10** minus **7M Na//2S//2O//3 (0. 1 ppm) gave cracking. With boric acid added, higher concentrations (1 ppm) were required. The SCC was electrochemically controlled. Below -0. 5 V//S//C//E (-0. 75//S//H//E), no SCC took place; above this potential, the rate increased with potential. Straining was required before SCC continued at 0. 5 v if the potential was held at or below -0. 5 v for extended times.
引用
收藏
页码:130 / 136
页数:7
相关论文
共 19 条
[1]   OCCURRENCE OF SALT FILMS DURING INITIATION AND GROWTH OF CORROSION PITS [J].
BECK, TR ;
ALKIRE, RC .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1979, 126 (10) :1662-1666
[2]  
BROPHY AJ, 1974, MAT PERF MAY, P9
[3]  
CLARKE WL, 1973, CORROSION, V29, P1, DOI 10.5006/0010-9312-29.1.1
[4]  
Cowan LR., 1973, ADV CORROS SCI TECH, V3, P293
[5]  
COWAN RL, 1977, NACE5 NAT ASS CORR E, P1023
[7]  
Dravnieks A., 1957, P API, V37, P100
[9]   CORROSION OF MATERIALS IN REACTOR CONTAINMENT SPRAY SOLUTIONS [J].
GRIESS, JC ;
BACARELL.AL .
NUCLEAR TECHNOLOGY, 1971, 10 (04) :546-&