INDENTATION DEFORMATION AND FRACTURE OF SAPPHIRE

被引:69
作者
CHAN, HM
LAWN, BR
机构
关键词
D O I
10.1111/j.1151-2916.1988.tb05756.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
引用
收藏
页码:29 / 35
页数:7
相关论文
共 31 条
[1]   A CRITICAL-EVALUATION OF INDENTATION TECHNIQUES FOR MEASURING FRACTURE-TOUGHNESS .1. DIRECT CRACK MEASUREMENTS [J].
ANSTIS, GR ;
CHANTIKUL, P ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (09) :533-538
[2]  
BECHER PF, 1976, J AM CERAM SOC, V59, P59, DOI 10.1111/j.1151-2916.1976.tb09390.x
[3]  
Cannon R, 1984, ADV CERAM, V10, P818
[4]   A CRITICAL-EVALUATION OF INDENTATION TECHNIQUES FOR MEASURING FRACTURE-TOUGHNESS .2. STRENGTH METHOD [J].
CHANTIKUL, P ;
ANSTIS, GR ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (09) :539-543
[5]  
COTTRELL AH, 1958, T AM I MIN MET ENG, V212, P192
[6]   STRENGTH AND FATIGUE PROPERTIES OF OPTICAL-GLASS FIBERS CONTAINING MICROINDENTATION FLAWS [J].
DABBS, TP ;
LAWN, BR .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1985, 68 (11) :563-569
[7]   FRACTURE TOUGHNESS DETERMINATIONS BY INDENTATION [J].
EVANS, AG ;
CHARLES, EA .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1976, 59 (7-8) :371-372
[8]   THEORY OF FATIGUE FOR BRITTLE FLAWS ORIGINATING FROM RESIDUAL-STRESS CONCENTRATIONS [J].
FULLER, ER ;
LAWN, BR ;
COOK, RF .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1983, 66 (05) :314-321
[9]   SHEAR DEFORMATION UNDER PYRAMIDAL INDENTATIONS IN SODA-LIME GLASS [J].
HAGAN, JT .
JOURNAL OF MATERIALS SCIENCE, 1980, 15 (06) :1417-1424
[10]   ORIGIN OF MEDIAN AND LATERAL CRACKS AROUND PLASTIC INDENTS IN BRITTLE MATERIALS [J].
HAGAN, JT ;
SWAIN, MV .
JOURNAL OF PHYSICS D-APPLIED PHYSICS, 1978, 11 (15) :2091-+