摘要
This study investigated the effect of wheat straw ash on the durability of concrete to freeze-thaw deterioration. Three wheat straw ash replacement levels were considered in the study: 5, 10 and 15% by weight of cement. The other experimental parameters investigated in the study included: aggregate type (basalt and pumice), water/binder ratio (0.5 and 0.7) and maximum aggregate size (9.5 and 19 mm). After the initial moist curing, wheat straw ash concrete prisms were subjected to accelerated freeze-thaw cycles following ASTM Procedure B (rapid freezing in air and thawing in water). The freeze-thaw deterioration of wheat straw ash concrete specimens was evaluated using the relative dynamic modulus of elasticity and durability factor. The results showed that the durability of wheat straw ash concrete to freeze-thaw deterioration was greater than that of plain concrete. Furthermore, the durability of wheat straw ash concrete to freeze-thaw deterioration increased with increasing wheat straw ash replacement level. The concrete containing pumice aggregate showed higher durability to freeze-thaw deterioration in comparison with that containing basalt aggregate. The effect of aggregate type was more pronounced for the wheat straw ash concrete than for plain concrete. The concrete at water/binder ratio of 0.5 showed higher durability to freeze-thaw deterioration than that at water/binder ratio of 0.7. The effect of water/binder ratio was more pronounced for the wheat straw ash concrete in comparison with the control concrete. Furthermore, the concrete with maximum aggregate size of 9.5 mm showed higher durability to freeze-thaw deterioration than concrete with maximum aggregate size of 19 mm.
引用
收藏
页码:79 / 86
页数:8
相关论文
共 50 条
  • [31] Effect of freeze-thaw cycles on the mechanical performance of wheat straw biomass ash modified soil
    Chen, Zhengfa
    Liu, Xibin
    Li, Quanmin
    Wu, Heng
    Zhang, Jiahao
    COLD REGIONS SCIENCE AND TECHNOLOGY, 2024, 222
  • [32] Durability and damage model of polyacrylonitrile fiber reinforced concrete under freeze-thaw and erosion
    Duan, Minghan
    Qin, Yuan
    Li, Yang
    Zhou, Heng
    CONSTRUCTION AND BUILDING MATERIALS, 2023, 394
  • [33] Fracture Behavior of Concrete Exposed to the Freeze-Thaw Environment
    Ma, Zhiming
    Zhao, Tiejun
    Yang, Jing
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2017, 29 (08)
  • [34] On Deterioration Mechanism of Concrete Exposed to Freeze-Thaw Cycles
    Trofimov, B. Ya
    Kramar, L. Ya
    Schuldyakov, K. V.
    INTERNATIONAL CONFERENCE ON CONSTRUCTION, ARCHITECTURE AND TECHNOSPHERE SAFETY (ICCATS 2017), 2017, 262
  • [35] Durability of concrete exposed to combined freeze-thaw, sulfate, and acid attacks after two years
    Tanyildizi, Harun
    REVISTA DE LA CONSTRUCCION, 2023, 22 (01): : 102 - 121
  • [36] Preliminary Study on Natural Freeze-thaw Pretreatment of Wheat straw
    Yu, Meng
    Wang, Lianjie
    Wang, Xinming
    ADVANCES IN CHEMICAL ENGINEERING II, PTS 1-4, 2012, 550-553 : 472 - 475
  • [37] A PERFORMANCE-BASED APPROACH TO CONCRETE FREEZE-THAW DURABILITY
    Song, Yu
    Das, Arnesh
    Lange, David A.
    Mosavi, Hossein
    Riding, Kyle
    PROCEEDINGS OF THE ASME JOINT RAIL CONFERENCE, 2018, 2018,
  • [38] Freeze-thaw durability of concrete: Ice formation process in pores
    Tsinghua Univ, Beijing, China
    Cem Concr Res, 9 (1281-1287):
  • [39] Optimal mix and freeze-thaw durability of polysulfide polymer concrete
    Hong, Sungnam
    Kim, Hyeonjun
    Park, Sun-Kyu
    CONSTRUCTION AND BUILDING MATERIALS, 2016, 127 : 539 - 545
  • [40] Freeze-thaw durability of recycled concrete containing ceramic aggregate
    Medina, Cesar
    Sanchez de Rojas, Maria Isabel
    Frias, Moises
    JOURNAL OF CLEANER PRODUCTION, 2013, 40 : 151 - 160