Analytical Investigation of Urea Deposits in SCR System

被引:43
作者
Weeks, Colin L. [1 ]
Ibeling, Dan R. [1 ]
Han, Sonia [1 ]
Ludwig, Lindsey [1 ]
Ayyappan, Ponnaiyan [2 ]
机构
[1] Univ Northern Iowa, Cedar Falls, IA 50614 USA
[2] John Deere Power Syst, Cedar Falls, IA USA
关键词
Ammonia - Deposits - Metabolism - Nitrogen oxides - Selective catalytic reduction - Catalysts - Decomposition - Thermogravimetric analysis - Exhaust gases - Ultraviolet visible spectroscopy;
D O I
10.4271/2015-01-1037
中图分类号
U [交通运输];
学科分类号
08 ; 0823 ;
摘要
An aqueous urea solution is used as the source of ammonia for selective catalytic reduction (SCR) of NOx to reduce the emissions of NOx in the exhaust of diesel vehicles. However, the decomposition of urea into ammonia is not always complete, resulting in solid urea deposit formation in the decomposition tube or on the SCR catalyst. These solid deposits can impede the flow of the exhaust gases (and uniformity of NH3 supply) and reduce SCR catalyst performance over time. To minimize the formation of urea deposit and to meet EPA NOx emission regulations, it is important to understand the chemistry of formation or removal of the deposit in the decomposition tube and SCR catalyst. In this report, IR spectroscopy, UV-visible spectroscopy, thermogravimetric analysis and elemental analysis have been used to determine the chemical composition of the solid urea deposits formed by the thermal decomposition of urea. Small and bulk urea deposit samples that formed during engine dyno tests with exhaust temperatures between 200 and 425 degrees C were analyzed. The results showed that exhaust temperatures of 200-250 degrees C inside the decomposition tube yielded unreacted urea, biuret and cyanuric acid. However their proportions varied appreciably from test to test. At exhaust temperatures of 335-425 degrees C, the deposits consist of mostly cyanuric acid. Small scale tests results revealed that urea, biuret and cyanuric acid in the solid urea deposits were not completely removed even though the exhaust temperature exceeded the temperatures at which these compounds thermally decompose.
引用
收藏
页码:1219 / 1239
页数:21
相关论文
共 15 条
[1]  
Bellamy L.J., 1975, LONDON
[2]   Ionothermal Synthesis of Crystalline, Condensed, Graphitic Carbon Nitride [J].
Bojdys, Michael J. ;
Mueller, Jens-Oliver ;
Antonietti, Markus ;
Thomas, Arne .
CHEMISTRY-A EUROPEAN JOURNAL, 2008, 14 (27) :8177-8182
[3]   THERMAL-BEHAVIOR OF MELAMINE [J].
COSTA, L ;
CAMINO, G .
JOURNAL OF THERMAL ANALYSIS, 1988, 34 (02) :423-429
[4]  
Dong H., 2008, 2008011544 SAE, DOI [10.4271/2008-01-1544, DOI 10.4271/2008-01-1544]
[5]  
EPA U, 2004, FED REG, V69, P38958
[6]   Urea thermolsis and NOx reduction with and without SCR catalysts [J].
Fang, HL ;
DaCosta, HFM .
APPLIED CATALYSIS B-ENVIRONMENTAL, 2003, 46 (01) :17-34
[7]   Urea and urea-water solutions-an infrared study [J].
Grdadolnik, J ;
Maréchal, Y .
JOURNAL OF MOLECULAR STRUCTURE, 2002, 615 (1-3) :177-189
[8]   Hydrolysis of isocyanic acid on SCR catalysts [J].
Kleemann, M ;
Elsener, M ;
Koebel, M ;
Wokaun, A .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2000, 39 (11) :4120-4126
[9]   Urea thermolysis studied under flow reactor conditions using DSC and FT-IR [J].
Lundstrom, Andreas ;
Andersson, Bengt ;
Olsson, Louise .
CHEMICAL ENGINEERING JOURNAL, 2009, 150 (2-3) :544-550
[10]   INFRARED SPECTRA OF CYANURIC ACID AND DEUTERO CYANURIC ACID [J].
NEWMAN, R ;
BADGER, RM .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 1952, 74 (14) :3545-3548