Unbonded Post Tensioned Concrete Slabs in Fire - Part I - Experimental Response of Unbonded Tendons under Transient Localized Heating

被引:15
作者
Gales, John
Bisby, Luke A. [1 ]
Gillie, Martin [2 ]
机构
[1] Ove Arup Fdn, Bronx, NY 10463 USA
[2] Univ Edinburgh, BRE Ctr Fire Safety Engn, Edinburgh EH9 3JL, Midlothian, Scotland
基金
英国工程与自然科学研究理事会; 加拿大自然科学与工程研究理事会;
关键词
Prestressing steel; Post-tensioned slabs; Unbonded construction; Fire endurance testing; Spalling; Concrete; Concrete cover; High temperature creep; Stress relaxation;
D O I
10.1260/2040-2317.2.3.139
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The fire-safe structural design and construction of unbonded post-tensioned (UPT) flat plate concrete structures has recently come under debate in the UK, and questions are being raised regarding the response to fire of post-tensioned concrete slabs. Related to these concerns is the real world response of continuous UPT tendons inside such structures both during and after a fire, which is largely unknown and depends on many potentially important factors which are not currently accounted for in standard fire tests. Several credible concerns exist for UPT concrete structures in fire, most notably the potential for premature tendon rupture due to localized heating which may result from a number of possible causes (discussed herein). The research presented in this paper deals specifically with the time-temperature-stress-strength interdependencies of stressed UPT tendons under localized transient heating, as may be experienced by tendons in a real UPT building in a real fire. Nineteen high temperature stress relaxation tests on UPT tendons of realistic length and parabolic longitudinal profile are reported. It is shown that localized heating of UPT tendons is likely to induce premature tendon rupture during fire, even in structures which meet the prescriptive concrete cover requirements imposed by available design codes.
引用
收藏
页码:139 / 153
页数:15
相关论文
共 41 条
[1]  
Abrams M. S., 1961, J PCA RES DEV LAB, V3, P8
[2]  
ACI:318, 2015, BUILDING CODE REQUIR
[3]  
[Anonymous], 2010, REINFORCED CONCRETE
[4]  
Bailey C, 2009, J STRUCT ENG, V87, P23
[5]   Fire tests on unbonded post-tensioned one-way concrete slabs [J].
Bailey, C. G. ;
Ellobody, E. .
MAGAZINE OF CONCRETE RESEARCH, 2009, 61 (01) :67-76
[6]   Whole-building behaviour of bonded post-tensioned concrete floor plates exposed to fire [J].
Bailey, Colin G. ;
Ellobody, Ehab .
ENGINEERING STRUCTURES, 2009, 31 (08) :1800-1810
[7]  
BARTH F, 1992, CONTROLLED DEMOLITIO
[8]  
British Standards Institution, 2002, EUR 2 DES CONCR STRU
[9]  
British Standards Institution, 2004, ENV199212 BRIT STAND
[10]  
Canadian Standards Association, 2004, CANCSAA23304