ELECTROPOTENTIAL INSPECTION OF SURFACE DEFECT DEPTH ON COMPONENTS MADE OF CARBON-GRAPHITE COMPOSITES

被引:0
作者
SOPILNIK, AV
REDKO, VI
机构
来源
SOVIET JOURNAL OF NONDESTRUCTIVE TESTING-USSR | 1990年 / 26卷 / 09期
关键词
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
An electropotential device for measuring the depth of surface cracks in components made of weakly conducting composites is presented. This device automatically does away with contact phenomena and variations in the electrical conductivity from section to section of the surface under study.
引用
收藏
页码:662 / 665
页数:4
相关论文
共 50 条
[1]   STRENGTH OF MODIFIED CARBON-GRAPHITE COMPOSITES [J].
BOLOTINA, KS ;
SHCHUGOREV, VN .
MECHANICS OF COMPOSITE MATERIALS, 1994, 30 (04) :378-381
[2]   High temperature graphite adhesive for carbon-graphite composites [J].
不详 .
INDUSTRIAL CERAMICS, 1999, 19 (03) :218-218
[3]   Strength of modified carbon-graphite composites [J].
Bolotina, K.S. ;
Shchugorev, V.N. .
Mekhanika Kompozitnykh Materialov, 1994, 30 (04) :520-525
[4]   Depth of the reaction of carbon-graphite materials with air [J].
Orenbakh, M.S. ;
Umrilova, N.M. .
Solid Fuel Chemistry, 1988, 22 (03) :99-103
[5]   INFLUENCE OF MICROSTRUCTURE ON MECHANICAL PROPERTIES OF CARBON-GRAPHITE MATRIX COMPOSITES [J].
MEYER, RA ;
EITMAN, DA ;
EVANGELI.JS .
CARBON, 1972, 10 (03) :334-&
[6]   Fracture toughness of pyrolytic carbon-graphite composites for biological applications [J].
Raguso, M ;
Casadei, A ;
Rossetto, M ;
Doglione, R ;
Firrao, D .
ECF 12: FRACTURE FROM DEFECTS, VOLS. I-III, 1998, :1387-1392
[7]   Superior mechanical properties of sulfonated graphene reinforced carbon-graphite composites [J].
Tu, Chuanjun ;
Hong, Lirui ;
Song, Tenghui ;
Li, Xuanke ;
Dou, Qinbao ;
Ding, Yichao ;
Liao, Tingting ;
Zhang, Sisi ;
Gao, Guoqiang ;
Wang, Ziqiu ;
Jiang, Yonghua .
CARBON, 2019, 148 :378-386
[8]   Carbide Formation at a Carbon-Graphite Lining Cathode Surface Wettable with Aluminum [J].
E. S. Gorlanov ;
V. Yu. Bazhin ;
S. N. Fedorov .
Refractories and Industrial Ceramics, 2016, 57 :292-296
[9]   Carbide Formation at a Carbon-Graphite Lining Cathode Surface Wettable with Aluminum [J].
Gorlanov, E. S. ;
Bazhin, V. Yu. ;
Fedorov, S. N. .
REFRACTORIES AND INDUSTRIAL CERAMICS, 2016, 57 (03) :292-296
[10]   DEVELOPMENT AND STUDY OF CARBON-GRAPHITE HEAVILY PLASMA-LOADED MICROWAVE COMPONENTS [J].
SKIBENKO, AI ;
VOITSENYA, VS ;
PAVLICHENKO, RO ;
TERESHIN, VI ;
FOMIN, IP ;
CHEBOTAREV, VV .
PLASMA PHYSICS REPORTS, 1994, 20 (02) :214-216