LOW-AMPLITUDE RECIPROCATING WEAR OF SINTERED IRON

被引:11
作者
LEHEUP, ER [1 ]
ZHANG, D [1 ]
MOON, JR [1 ]
机构
[1] UNIV NOTTINGHAM,DEPT MAT ENGN & MAT DESIGN,NOTTINGHAM NG7 2RD,ENGLAND
关键词
Wear of materials;
D O I
10.1016/0043-1648(94)90205-4
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The unlubricated wear, self-on-self, of sintered iron due to reciprocating motion has been investigated. Wrought, low-carbon steel have also been studied under identical conditions for comparison. The general characteristics of the wear process for the sintered material are similar to those observed for wrought material. Wear is more severe when the load is increased and when the amplitude is increased in the range up to about 250 mum. Further increases in amplitude brought about less marked increases in wear, until, ultimately, wear became independent of amplitude. At high sliding speeds, sintered iron loses more weight than does mild steel. At slow speeds, sintered iron loses weight less rapidly than does mild steel. The observations are interpreted in the light of oxide formation on the bearing surfaces and of observations of wear debris accumulated in surface breaking pores.
引用
收藏
页码:121 / 130
页数:10
相关论文
共 13 条
  • [1] FRETTING - LOAD CARRYING-CAPACITY OF WEAR DEBRIS
    COLOMBIE, C
    BERTHIER, Y
    FLOQUET, A
    VINCENT, L
    GODET, M
    [J]. JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 1984, 106 (02): : 194 - 201
  • [2] EYRE TS, 1976, POWDER METALL, V1, P22
  • [3] THE 3RD-BODY APPROACH - A MECHANICAL VIEW OF WEAR
    GODET, M
    [J]. WEAR, 1984, 100 (1-3) : 437 - 452
  • [4] THE INFLUENCE OF SPEED ON THE WEAR OF SINTERED IRON-BASED MATERIALS
    GOPINATH, K
    [J]. WEAR, 1981, 71 (02) : 161 - 178
  • [5] FRICTION AND WEAR OF SINTERED IRON
    GOPINATH, K
    RAYUDU, GVN
    NARAYANAMURTHI, RG
    [J]. WEAR, 1977, 42 (02) : 245 - 250
  • [6] FRETTING WEAR OF MILD-STEEL FROM ROOM-TEMPERATURE TO 200 DEGREES C
    HURRICKS, PL
    [J]. WEAR, 1972, 19 (02) : 207 - &
  • [7] EFFECT OF THE HARDNESS OF HARDENED STEELS AND THE ACTION OF OXIDES ON FRETTING WEAR
    KAYABA, T
    IWABUCHI, A
    [J]. WEAR, 1981, 66 (01) : 27 - 41
  • [8] KUNO M, 1989, 5TH P INT C TRIB HEL, V3, P30
  • [9] UNLUBRICATED RECIPROCATING WEAR OF STAINLESS-STEEL WITH AN INTERFACIAL AIR-FLOW
    LEHEUP, ER
    PENDLEBURY, RE
    [J]. WEAR, 1991, 142 (02) : 351 - 372
  • [10] THE UNLUBRICATED WEAR OF SINTERED IRON
    LIM, SC
    BRUNTON, JH
    [J]. WEAR, 1986, 113 (03) : 371 - 382