HYDROGEN-IMPLANTED AND HELIUM-IMPLANTED SILICON - LOW-TEMPERATURE POSITRON-LIFETIME STUDIES

被引:6
|
作者
MAKINEN, S [1 ]
RAJAINMAKI, H [1 ]
LINDEROTH, S [1 ]
机构
[1] TECH UNIV DENMARK,APPL PHYS LAB,DK-2800 LYNGBY,DENMARK
来源
PHYSICAL REVIEW B | 1991年 / 44卷 / 11期
关键词
D O I
10.1103/PhysRevB.44.5510
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
High-purity single-crystal samples of float-zoned Si have been implanted with 6.95-MeV protons and with 25-MeV He-3(2) ions at 15 K, and the positron-lifetime technique has been used to identify the defects created in the samples, and to study the effects of H and He on the annealing of point defects in Si. The results have been compared with those of proton-irradiated Si. A 100-300-K annealing stage was clearly observed in hydrogen (H+) -implanted Si, and this stage was almost identical to that in the p-irradiated Si. The final annealing state of the H+-implanted Si started at about 400 K, and it is connected to annealing out of negatively charged divacancy-oxygen pairs. This stage was clearly longer than that for the p-irradiated Si, probably due to the breakup of Si-H bonds at about 550 K. The 100-K annealing stage was not seen with the He-implanted samples. This has been explained by assuming that almost all vacancies contained He after the irradiation with He-3. Helium is suggested to be released from vacancies at about 600 K, and small He bubbles seem to have grown at temperatures above 800 K. The specific positron-trapping rate for negatively charged monovacancy-type defects in H+-implanted Si has been found to have a T-0.5 dependence, whereas for neutral divacancies and monovacancies in He-implanted Si no dependence on temperature has been observed.
引用
收藏
页码:5510 / 5517
页数:8
相关论文
共 50 条
  • [22] Temperature Dependence of Defects in Hydrogen-Implanted Silicon Characterized by Positron and Ion-Beam Analyses
    Kinomura, A.
    Suzuki, R.
    Ohdaira, T.
    Muramatsu, M.
    He, C.
    Oshima, N.
    Matsumoto, T.
    Horino, Y.
    POSITRON STUDIES OF DEFECTS 2011, 2012, 35 : 151 - 156
  • [23] TEMPERATURE AND DOSE DEPENDENCE OF DAMAGE ACCUMULATION IN HYDROGEN-IMPLANTED SILICON
    HALL, BO
    JOURNAL OF METALS, 1985, 37 (08): : A21 - A21
  • [24] High temperature indentation of helium-implanted tungsten
    Gibson, James S. K. -L.
    Roberts, Steve G.
    Armstrong, David E. J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 625 : 380 - 384
  • [25] METASTABLE DEFECT STATES IN HYDROGEN-IMPLANTED SILICON
    GORELKINSKII, YV
    NEVINNYI, NN
    RADIATION EFFECTS AND DEFECTS IN SOLIDS, 1983, 71 (1-2): : 1 - 8
  • [26] Shallow donor formation in hydrogen-implanted silicon
    Tokuda, Y
    Iwata, H
    Ito, A
    DEFECTS IN ELECTRONIC MATERIALS II, 1997, 442 : 205 - 210
  • [27] Biomimetic growth of apatite on hydrogen-implanted silicon
    Liu, XY
    Fu, RKY
    Poon, RWY
    Chen, P
    Chu, PK
    Ding, CX
    BIOMATERIALS, 2004, 25 (25) : 5575 - 5581
  • [28] DEPTH DISTRIBUTIONS OF HYDROGEN-IMPLANTED AND ANNEALED SILICON
    WILSON, RG
    APPLIED PHYSICS LETTERS, 1986, 49 (20) : 1375 - 1377
  • [29] Low temperature exfoliation process in hydrogen-implanted germanium layers
    Ferain, I. P.
    Byun, K. Y.
    Colinge, C. A.
    Brightup, S.
    Goorsky, M. S.
    JOURNAL OF APPLIED PHYSICS, 2010, 107 (05)
  • [30] Trapping of hydrogen impurities in helium-implanted niobium and tantalum
    1600, American Inst of Physics, Woodbury, NY, USA (75):