Impact-sliding fretting tribocorrosion behavior of 316L stainless steel in solution with different halide concentrations

被引:0
作者
Xu Ma
Wei Tan
Remy Bonzom
Xue Mi
Guorui Zhu
机构
[1] Tianjin University,School of Chemical Engineering and Technology
[2] Zhejiang Institute of Tianjin University,Materials and Mechanics of Components Department
[3] Electricité de France R&D,undefined
[4] Nuclear Power Institute of China,undefined
来源
Friction | 2023年 / 11卷
关键词
impact-sliding; fretting wear; tribocorrosion; halide concentration; 316L stainless steel;
D O I
暂无
中图分类号
学科分类号
摘要
Impact-sliding caused by random vibrations between tubes and supports can affect the operation of heat exchangers. In addition, a corrosive environment can cause damage, accelerating the synergism of corrosion and wear. Therefore, the focus of this work was the impact-sliding fretting tribocorrosion behavior of 316L heat exchanger tubes at different halide concentrations. A device system incorporating the in situ electrochemical measurements of impact-sliding fretting corrosion wear was constructed, and experiments on 316L heat exchanger tubes in sodium chloride (NaCl) solution with different concentrations (0.0, 0.1, 0.5, 1.0, 3.5, and 5.0 wt%) were carried out. The synergism between wear and corrosion was also calculated and analyzed. The wear and damage mechanisms were elucidated by correlating the corrosion-wear synergism, morphologies, and material loss rates. The results indicated that the stable wear stage occurred at approximately 9–12 h, after which the corrosion current increased with the expansion of the wear area. As the halide concentration increased, the scale of damage on the wear scars gradually decreased, changing from being dominated by cracks, delaminations, and grooves to being dominated by scratches, microgrooves, and holes. There was an obvious positive synergism between wear and corrosion. The material loss was dominated by pure mechanical wear and wear enhanced by corrosion, but corrosion enhanced by wear contributed more than tangential sliding fretting corrosion. The total mass loss increased gradually in the range of 0.0–0.5 wt% and decreased in the range of 0.5–5.0 wt%. Large-scale damage enhanced by corrosivity and small-scale damage reduced by lubricity dominated the material loss at low and high concentrations, respectively.
引用
收藏
页码:2310 / 2328
页数:18
相关论文
共 43 条
[31]   Tribocorrosion behavior of nickel-aluminium bronze sliding against alumina under the lubrication by seawater with different halide concentrations [J].
Zhang, Beibei ;
Wang, Jianzhang ;
Yuan, Junya ;
Yan, Fengyuan .
FRICTION, 2019, 7 (05) :444-456
[32]   Tribocorrosion behavior of nickel-aluminium bronze sliding against alumina under the lubrication by seawater with different halide concentrations [J].
Beibei ZHANG ;
Jianzhang WANG ;
Junya YUAN ;
Fengyuan YAN .
Friction, 2019, 7 (05) :444-456
[33]   Tribocorrosion behavior of nickel-aluminium bronze sliding against alumina under the lubrication by seawater with different halide concentrations [J].
Beibei Zhang ;
Jianzhang Wang ;
Junya Yuan ;
Fengyuan Yan .
Friction, 2019, 7 :444-456
[34]   Tribocorrosion of 316L stainless steel and TA6V4 alloy in H2SO4 media [J].
Henry, P. ;
Takadoum, J. ;
Bercot, P. .
CORROSION SCIENCE, 2009, 51 (06) :1308-1314
[35]   Effect of frictional frequency on the subsurface evolution of 316L stainless steel in tribocorrosion and its influence on the synergistic effect between corrosion and wear [J].
Wu, Yinchao ;
Wang, Zhongwei ;
Chen, Jiaolong ;
Ma, Yanlong ;
Yan, Yu ;
Qiao, Lijie .
TRIBOLOGY INTERNATIONAL, 2023, 178
[36]   Response of duplex Cr(N)/S and Cr(C)/S coatings on 316L stainless steel to tribocorrosion in 0.89% NaCl solution under plastic contact conditions [J].
Sun, Y. ;
Dearnley, P. A. ;
Mallia, Bertram .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2017, 105 (06) :1503-1513
[37]   Tribocorrosion of 316L stainless steel by in-situ electrochemical methods under deep-sea high hydrostatic pressure environment [J].
Ren, Pengwei ;
Meng, Huimin ;
Xia, Qijun ;
Zhu, Zhongzheng ;
He, Mingtao .
CORROSION SCIENCE, 2022, 202
[38]   Three-Body Abrasion-Corrosion Behavior of As-Printed and Solution-Annealed Additively Manufactured 316L Stainless Steel [J].
Salasi, Mobin ;
Wang, Ke ;
Pojtanabuntoeng, Thunyaluk ;
Pabbruwe, Moreica ;
Quadir, Zakaria ;
Rickard, William ;
Guagliardo, Paul ;
Iannuzzi, Mariano .
CORROSION, 2022, 78 (05) :390-403
[39]   Development of tribological maps on borided AISI 316L stainless steel under ball-on-flat wet sliding conditions [J].
Garcia-Leon, R. A. ;
Martinez-Trinidad, J. ;
Campos-Silva, I ;
Figueroa-Lopez, U. ;
Guevara-Morales, A. .
TRIBOLOGY INTERNATIONAL, 2021, 163
[40]   Tribocorrosion performance of 316L stainless steel enhanced by laser clad 2-layer coating using Fe-based amorphous powder [J].
Ji, Xiulin ;
Luo, Chanyuan ;
Jin, Juan ;
Zhang, Yingtao ;
Sun, Yong ;
Fu, Li .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 17 :612-621