Impact-sliding fretting tribocorrosion behavior of 316L stainless steel in solution with different halide concentrations

被引:0
作者
Xu Ma
Wei Tan
Remy Bonzom
Xue Mi
Guorui Zhu
机构
[1] Tianjin University,School of Chemical Engineering and Technology
[2] Zhejiang Institute of Tianjin University,Materials and Mechanics of Components Department
[3] Electricité de France R&D,undefined
[4] Nuclear Power Institute of China,undefined
来源
Friction | 2023年 / 11卷
关键词
impact-sliding; fretting wear; tribocorrosion; halide concentration; 316L stainless steel;
D O I
暂无
中图分类号
学科分类号
摘要
Impact-sliding caused by random vibrations between tubes and supports can affect the operation of heat exchangers. In addition, a corrosive environment can cause damage, accelerating the synergism of corrosion and wear. Therefore, the focus of this work was the impact-sliding fretting tribocorrosion behavior of 316L heat exchanger tubes at different halide concentrations. A device system incorporating the in situ electrochemical measurements of impact-sliding fretting corrosion wear was constructed, and experiments on 316L heat exchanger tubes in sodium chloride (NaCl) solution with different concentrations (0.0, 0.1, 0.5, 1.0, 3.5, and 5.0 wt%) were carried out. The synergism between wear and corrosion was also calculated and analyzed. The wear and damage mechanisms were elucidated by correlating the corrosion-wear synergism, morphologies, and material loss rates. The results indicated that the stable wear stage occurred at approximately 9–12 h, after which the corrosion current increased with the expansion of the wear area. As the halide concentration increased, the scale of damage on the wear scars gradually decreased, changing from being dominated by cracks, delaminations, and grooves to being dominated by scratches, microgrooves, and holes. There was an obvious positive synergism between wear and corrosion. The material loss was dominated by pure mechanical wear and wear enhanced by corrosion, but corrosion enhanced by wear contributed more than tangential sliding fretting corrosion. The total mass loss increased gradually in the range of 0.0–0.5 wt% and decreased in the range of 0.5–5.0 wt%. Large-scale damage enhanced by corrosivity and small-scale damage reduced by lubricity dominated the material loss at low and high concentrations, respectively.
引用
收藏
页码:2310 / 2328
页数:18
相关论文
共 40 条
  • [21] Effect of electrochemical potential on tribocorrosion behavior of low temperature plasma carburized 316L stainless steel in 1 M H2SO4 solution
    Sun, Y.
    Haruman, E.
    SURFACE & COATINGS TECHNOLOGY, 2011, 205 (17-18) : 4280 - 4290
  • [22] Effect of the third body layer formed at different temperature on fretting wear behavior of 316 stainless steel in the composite fretting motion of slip and impact
    Zhang, Shengzan
    Liu, Liyan
    Ma, Xu
    Zhu, Guorui
    Tan, Wei
    WEAR, 2022, 492-493
  • [23] The effect of the substrate surface state on the morphology, topography and tribocorrosion behavior of Si/Zr sol-gel coated 316L stainless steel
    Kossman, Stephania
    Coelho, Leonardo Bertolucci
    Montagne, Alex
    Mejias, Alberto
    Van Gorp, Adrien
    Coorevits, Thierry
    Touzin, Matthieu
    Druart, Marie-Eve
    Staia, Mariana H.
    Poorteman, Marc
    Olivier, Marie-Georges
    SURFACE & COATINGS TECHNOLOGY, 2021, 406
  • [24] Tribocorrosion and corrosion behavior of stainless steel coated with DLC films in ethanol with different concentrations of water
    Radi, Polyana Alves
    Vieira, Angela
    Manfroi, Lucas
    de Farias Nass, Karina Carvalho
    Ramirez Ramos, Marco Antonio
    Leite, Priscila
    Martins, Gislene Valdete
    Freire Jofre, Jorge Benedito
    Vieira, Lucia
    CERAMICS INTERNATIONAL, 2019, 45 (07) : 9686 - 9693
  • [25] Contact geometry and contact time effect on 690TT alloy/405 stainless steel impact-sliding fretting wear processes
    Mi, Xue
    Tang, Pan
    Zhang, Jun
    Bai, Xiao-ming
    Sun, Qi
    Zhu, Min-hao
    WEAR, 2025, 562
  • [26] Tribocorrosion properties of plasma nitrided, Ti-DLC coated and duplex surface treated AISI 316L stainless steel
    Uzun, Y.
    SURFACE & COATINGS TECHNOLOGY, 2022, 441
  • [27] Role of gradient nano-structured surface in collapsed pitting corrosion on AISI 316L stainless steel during tribocorrosion
    Zou, Jingyi
    Wang, Zhongwei
    Ma, Yanlong
    Yan, Yu
    Qiao, Lijie
    CORROSION SCIENCE, 2022, 197
  • [28] Tribocorrosion behavior of nickel-aluminium bronze sliding against alumina under the lubrication by seawater with different halide concentrations
    Zhang, Beibei
    Wang, Jianzhang
    Yuan, Junya
    Yan, Fengyuan
    FRICTION, 2019, 7 (05) : 444 - 456
  • [29] Tribocorrosion behavior of nickel-aluminium bronze sliding against alumina under the lubrication by seawater with different halide concentrations
    Beibei ZHANG
    Jianzhang WANG
    Junya YUAN
    Fengyuan YAN
    Friction, 2019, 7 (05) : 444 - 456
  • [30] Tribocorrosion behavior of nickel-aluminium bronze sliding against alumina under the lubrication by seawater with different halide concentrations
    Beibei Zhang
    Jianzhang Wang
    Junya Yuan
    Fengyuan Yan
    Friction, 2019, 7 : 444 - 456