Characteristics of machined surface integrity in face milling Al-Li alloy 2A97 with carbide inserts

被引:1
作者
Jintao Niu
Zhanqiang Liu
Xing Ai
Weimin Huang
Guijie Wang
Ran Duan
机构
[1] Shandong University,Key Laboratory of High Efficiency and Clean Mechanical Manufacture of MOE, School of Mechanical Engineering
[2] Shandong University,Key National Demonstration Center for Experimental Mechanical Engineering Education
来源
The International Journal of Advanced Manufacturing Technology | 2019年 / 101卷
关键词
Al-Li alloy; Chip morphology; Tool insert worn morphology; Machined surface integrity;
D O I
暂无
中图分类号
学科分类号
摘要
2A97 is one of the latest generations of Al-Li alloys that can be widely applied in the aerospace field which always takes weight reduction into consideration. An experimental investigation was conducted to study the machined surface integrity characteristics in face milling 2A97 with cemented carbide inserts on the basis of Taguchi orthogonal method. The multi-surfaces of chips and the rake faces of inserts were characterized. The effects of cutting process parameters, namely the cutting speed, the feed rate per tooth, the depth and width of cut on the machined surface roughness and residual stresses, were found out through range analysis. The work hardening and microstructure of machined surface layer were analyzed. The research results revealed that severe plastic deformation was developed during the chip formation process. Micro-chippings that situated along cutting edges constituted worn morphology of carbide inserts. The feed rate per tooth fz and depth of cut ap were more important than the width of cut ae and cutting speed vc to the machined surface roughness. Work hardening with different levels and residual stresses with small magnitudes were found on these machined surfaces. Little change was observed in the cross-sectional microstructure. In general, the similar machined surface integrity characteristics were observed in face milling 2A97 and conventional aluminum alloys. This conclusion can provide the foundation for applying widely 2A97 in aerospace industry.
引用
收藏
页码:839 / 848
页数:9
相关论文
共 132 条
  • [1] Luo C(2016)Characterization of localized corrosion in an Al-Cu-Li alloy J Mater Eng Perform 25 1811-1819
  • [2] Zhang XX(2013)Texture evolution within the thermomechanically affected zone of an Al-Li alloy 2195 friction stir weld Metall Mater Trans A 44 4906-4913
  • [3] Zhou XR(2014)Investigation of surface integrity of aluminum lithium alloy in high speed machining (in Chinese) Sci Sin Technol 44 89-98
  • [4] Sun ZH(2015)Cryogenic milling of aluminum-lithium alloys: thermo-mechanical modelling towards fine-tuning of part surface residual stress Procedia CIRP 31 160-165
  • [5] Zhang XY(2016)Influence of machining parameters on heat generation during milling of aluminum alloys Procedia CIRP 46 39-42
  • [6] Tang ZH(2014)Effect of thermo-mechanical treatment process on microstructure and mechanical properties of 2A97 Al-Li alloy Trans Nonferrous Metals Soc China 24 2196-2202
  • [7] Lu F(2013)Effect of heat treatment process on tensile properties of 2A97 Al-Li alloy: experiment and BP neural network simulation Trans Nonferrous Metals Soc China 23 1728-1736
  • [8] Thompson GE(2016)Continuous and discontinuous localized corrosion of a 2xxx aluminium–copper–lithium alloy in sodium chloride solution J Alloys Compd 658 61-70
  • [9] Tayon WA(2014)Microstructure and mechanical properties of newly developed aluminum–lithium alloy 2A97 welded by fiber laser Mater Sci Eng A 617 1-11
  • [10] Domack MS(2015)Microstructure and mechanical properties of friction spot welding aluminium–lithium 2A97 alloy Mater Des 83 719-727