Corrosion Performance of AISI 304 Stainless Steel in CO2-Saturated Brine Solution

被引:0
|
作者
H. Ruiz-Luna
J. Porcayo-Calderón
A.G. Mora-García
I. López-Báez
L. Martinez-Gomez
J. Muñoz-Saldaña
机构
[1] Conacyt–Universidad Autónoma de Zacatecas,
[2] Universidad Autónoma del Estado de Morelos,undefined
[3] CIICAp,undefined
[4] Centro de Investigación y de Estudios Avanzados del I.P.N.,undefined
[5] Universidad de Guanajuato,undefined
[6] Ex–Hacienda San Matías s/n,undefined
[7] Instituto de Ciencias Físicas-UNAM,undefined
[8] Av. Universidad s/n Col. Chamilpa,undefined
来源
Protection of Metals and Physical Chemistry of Surfaces | 2019年 / 55卷
关键词
electrochemical corrosion; stainless steel; oxide layer; Cr content; surface morphology;
D O I
暂无
中图分类号
学科分类号
摘要
引用
收藏
页码:1226 / 1235
页数:9
相关论文
共 50 条
  • [1] Corrosion Performance of AISI 304 Stainless Steel in CO2-Saturated Brine Solution
    Ruiz-Luna, H.
    Porcayo-Calderon, J.
    Mora-Garcia, A. G.
    Lopez-Baez, I.
    Martinez-Gomez, L.
    Munoz-Saldana, J.
    PROTECTION OF METALS AND PHYSICAL CHEMISTRY OF SURFACES, 2019, 55 (06) : 1226 - 1235
  • [2] Corrosion Inhibition of Imidazoline Derivates with Benzene Rings on Mild Steel in CO2-Saturated Brine Solution
    CHEN Guo-hao and ZHAO Jing-mao * College of Materials Science and Engineering
    ChemicalResearchinChineseUniversities, 2012, 28 (04) : 691 - 695
  • [3] Corrosion Inhibition of Imidazoline Derivates with Benzene Rings on Mild Steel in CO2-Saturated Brine Solution
    Chen Guo-hao
    Zhao Jing-mao
    CHEMICAL RESEARCH IN CHINESE UNIVERSITIES, 2012, 28 (04) : 691 - 695
  • [4] Influence of temperature on corrosion behavior of additively manufactured SS316L stainless steel in CO2-saturated brine solution
    Ansari, Nooruddin
    Alabtah, Fatima Ghassan
    Khraisheh, Marwan
    MATERIALS LETTERS, 2024, 376
  • [5] Corrosion Inhibition of N80 Steel with the Presence of Asymmetric Gemini in a CO2-saturated Brine Solution
    Wang, Hu
    Tang, Jun
    Xie, Juan
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2017, 12 (11): : 11017 - 11029
  • [6] Dandelion-Root Extract as Green Corrosion Inhibitor for Carbon Steel in CO2-Saturated Brine Solution
    Zbulj, Katarina
    Hrncevic, Lidia
    Bilic, Gordana
    Simon, Katarina
    ENERGIES, 2022, 15 (09)
  • [7] Inhibition performance and adsorption behaviour of dodecylamine on N80 steel in CO2-saturated brine solution
    Lu Zhaoling
    Fu Chaoyang
    Guo Xingpeng
    ANTI-CORROSION METHODS AND MATERIALS, 2007, 54 (05) : 301 - 307
  • [8] Evaluation of corrosion inhibition at sand-deposited carbon steel in CO2-saturated brine
    Pandarinathan, Vedapriya
    Lepkova, Katerina
    Bailey, Stuart I.
    Gubner, Rolf
    CORROSION SCIENCE, 2013, 72 : 108 - 117
  • [9] Corrosion behavior of supermartensitic stainless steel in aerated and CO2-saturated synthetic seawater
    Anselmo, N.
    May, J. E.
    Mariano, N. A.
    Nascente, P. A. P.
    Kuri, S. E.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 428 (1-2): : 73 - 79
  • [10] CHARACTERISTICS OF CORROSION SCALES ON STEELS IN A CO2-SATURATED NACL BRINE
    PALACIOS, CA
    SHADLEY, JR
    CORROSION, 1991, 47 (02) : 122 - 127