Electrospun poly(l-lactic acid) fiber mats containing crude Garcinia mangostana extracts for use as wound dressings

被引:0
作者
Orawan Suwantong
Porntipa Pankongadisak
Suwanna Deachathai
Pitt Supaphol
机构
[1] Mae Fah Luang University,School of Science
[2] Chulalongkorn University,The Petroleum and Petrochemical College, The Center of Excellence on Petrochemical and Materials Technology
来源
Polymer Bulletin | 2014年 / 71卷
关键词
Poly(; -lactic acid); Electrospinning; Drug delivery systems; extract; Wound dressings;
D O I
暂无
中图分类号
学科分类号
摘要
Poly(l-lactic acid) (PLLA) fiber mats containing two types of crude Garcinia mangostana Linn. (GM) extract [i.e., dichloromethane extract (dGM) and acetone extract (aGM)] were successfully prepared by electrospinning process. Both the neat and the GM-loaded PLLA fibers were smooth, with the average diameters ranging between 0.77 and 1.14 μm. The release characteristics of GM from the GM-loaded PLLA fiber mats were carried out by total immersion method in acetate buffer or simulated body fluid that contained 0.5 % v/v Tween 80 and 3 % v/v methanol (hereafter, A/T/M or S/T/M medium) at either 32 or 37 °C, respectively. The maximum cumulative amounts of GM released from the GM-loaded PLLA fiber mats in the S/T/M medium were greater than those in the A/T/M medium. Moreover, the cumulative amounts of GM released from the aGM-loaded PLLA fiber mats were greater than those from the dGM-loaded PLLA fiber mats in both types of medium. The antibacterial activity of the dGM-loaded PLLA fiber mats was greatest against Staphylococcus aureus DMST 20654, while that of the aGM-loaded PLLA fiber mats was greatest against S. aureus ATCC 25923 and S. epidermidis. Lastly, only the dGM-loaded PLLA fiber mats at extraction ratio of 10 mg mL−1 were toxic to the human dermal fibroblasts.
引用
收藏
页码:925 / 949
页数:24
相关论文
共 239 条
[1]  
Hartgerink JD(2001)Self-assembly and mineralization of peptide-amphiphile nanofibers Science 294 1684-1688
[2]  
Beniash E(2003)Fabrication of novel biomaterials through molecular self-assembly Nat Biotechnol 21 1171-1178
[3]  
Stupp SI(2002)Peptide-amphiphile nanofibers: a versatile scaffold for the preparation of self-assembling materials Proc Natl Acad Sci USA 99 5133-5138
[4]  
Zhang S(2003)Structure and morphology changes during in vitro degradation of electrospun poly(glycolide-co-lactide) nanofiber membran Biomacromolecules 4 416-423
[5]  
Hargerink JD(2003)A biodegradable nanofiber scaffold by electrospinning and its potential for bone tissue engineering Biomaterials 24 2077-2082
[6]  
Beniash E(1996)Phase separation processes in polymer solutions in relation to membrane formation J Membr Sci 117 1-31
[7]  
Stupp SI(2006)Preparation of polymer blend hollow fiber membrane via thermally induced phase separation Sep Purif Technol 52 363-371
[8]  
Zong X(1996)Nanometre diameter fibres of polymer, produced by electrospinning Nanotechnology 7 216-223
[9]  
Ran S(2009)Highly porous fibers prepared by electrospinning a ternary system of nonsolvent/solvent/poly( Mater Lett 63 415-418
[10]  
Kim K-S(2009)-lactic acid) Carbohydr Polym 77 863-869