Mold Coatings to Reduce Graphite Degeneration in the Surface Layer of Ductile Iron Castings

被引:0
作者
N. Ivan
M. Chisamera
I. Riposan
机构
[1] Politehnica University of Bucharest,
来源
International Journal of Metalcasting | 2012年 / 6卷
关键词
ductile iron; surface layer; graphite degeneration; furan resin mold; active mold coating; Mg-bearing coating;
D O I
暂无
中图分类号
学科分类号
摘要
The performance of coatings for furan resin sand molds using P-Toluol Sulfonic Acid (PTSA) hardener was evaluated for a surface layer of degenerated graphite in ductile iron test castings. It was reconfirmed that sulfur delivered by this mold type is an important contributor to graphite degeneration, especially in castings exhibiting lower graphite nodularity. A no-coating condition and especially a S-bearing coating led to a thicker surface layer and decreased graphite nodularity in the entire casting section, while MgO or (CaO + MgO + Talc) or Mg-FeSi blended coatings had beneficial effects, increasing in the order written, with (Mg + FeSi) coating the best performance. The applied coatings act mainly to control chemical interactions, such as S with Mg (or RE) rather than controlling heat transfer. Mg in a coating can offset Mg loss in the casting beyond the role of MgO or (CaO + MgO + Talc) coatings to inhibit S migration from the mold. This complex behavior could justify the application of coatings incorporating active Mg, from a fine sized Mg-FeSi alloy.
引用
收藏
页码:61 / 70
页数:9
相关论文
共 54 条
  • [1] Riposan I(2010)Performance of Heavy Ductile Iron Castings for Windmills China Foundry 7 163-170
  • [2] Chisamera M(2008)Surface Graphite Degeneration in Ductile Iron Castings for Resin Molds Tsinghua Science and Technology Journal 13 157-163
  • [3] Stan S(2003)Static Mechanical Properties of Ferritic and Pearlitic Lightweight Ductile Iron Castings AFS Transactions 111 895-910
  • [4] Riposan I(2003)Production and Properties of Thin-wall Ductile Iron Castings International Journal of Cast Metals Research 16 313-318
  • [5] Chisamera M(2005)Controlling the Skin Effect on Thin-wall Ductile Iron Castings AFS Transactions 113 567-579
  • [6] Stan S(2008)Comparative Study of Fatigue Endurance Limit for 4 and 6 mm Thin Wall Ductile Iron Castings International Journal of Metalcasting 2 7-17
  • [7] Skaland T(2008)Quantification of Casting Skin in Ductile and Compacted Graphite Irons and its Effect on Tensile Properties International Journal of Metalcasting 2 7-26
  • [8] Dix LP(1979)Localized Flake Graphite Structure as a Result of a Reaction Between Molten Ductile Iron and Some Components of the Mold AFS Transactions 87 221-226
  • [9] Ruxanda R(1969)Behavior of Nitrogen in Cast Iron AFS Cast Metals Research Journal 5 109-15
  • [10] Torrance J(1992)Nodular Iron Surface Deterioration Due to PTSA in Resin AFS Transactions 100 9-300