Effect of Transition Metals Addition on Tensile Properties of Al–Si–Cu-Based Alloys at 25 °C and 250 °C: Role of Heat Treatment

被引:0
作者
L. Alyaldin
M. H. Abdelaziz
A. M. Samuel
H. W. Doty
F. H. Samuel
机构
[1] Université du Québec à Chicoutimi,Département des Sciences appliquées
[2] Université Française d’Égypte,Département PEC
[3] General Motors Materials Engineering,undefined
来源
International Journal of Metalcasting | 2021年 / 15卷
关键词
aluminum alloys; heat treatment; tensile properties; quality index; statistical analysis;
D O I
暂无
中图分类号
学科分类号
摘要
The tensile data showed that strength and percent elongation of the Zr-containing 354 (Al–9%Si–1.8%Cu–0.5%Mg) alloys increased in the one-step solution heat-treated condition compared to the as-cast case. The multi-step solution heat treatment displayed higher tensile properties than those achieved with single-step solution heat treatment. The use of the T6 treatment, incorporating the multiple solution heat treatment, allows for maximum dissolution of the copper phases in the multiple stages of solution treatment, resulting in the greatest improvement in the alloy strength. The best tensile properties of alloys tested at room temperature after stabilization at 250 °C for 200 h are obtained with the T6 heat treatment. The addition of Zr, Ni, and Mn to Al–Si alloys improves the high-temperature tensile properties of the 354 alloy. Alloys containing 2%Ni or 0.75%Mn perform better in case of high-temperature conditions, with 1-h stabilization at 250 °C. After 200-h stabilization at 250 °C, the strength of the T6-treated alloys—regardless of the type of solution heat treatment process, is reduced considerably, while the ductility is increased, with base alloy showing the highest percent elongation, ~ 19%. The reduction in strength may be attributed to the alloy softening which occurs after such long stabilization time at the high testing temperature (250 °C).
引用
收藏
页码:60 / 75
页数:15
相关论文
共 60 条
[1]  
Lemon R(1963)Premium strength aluminum casting alloys 354 and 359 Trans. AFS 71 465-2263
[2]  
Howle C(1994)Effect of heat treatment on the microstructure, tensile properties, and fracture behavior of permanent mold Al-10 Wt Pct Si-0.6 Wt Pct Mg/Sic/10 P composite castings Metall. Mater. Trans. A 25 2247-4697
[3]  
Samuel F(1999)Effect of Mg on the ageing behaviour of Al–Si–Cu 319 type aluminium-casting alloys J. Mater. Sci. 34 4671-298
[4]  
Samuel A(2005)Effect of copper and silicon content on mechanical properties in Al–Cu–Si–Mg alloys J. Mater. Process. Technol. 169 292-414
[5]  
Ouellet P(2018)Response of varying levels of silicon and transition elements on room- and elevated-temperature tensile properties in an Al–Cu alloy Int. J. Metalcast. 1 396-72
[6]  
Samuel FH(2013)Microstructure, tensile properties and fracture behavior of high temperature Al–Si–Mg–Cu cast alloys Mater. Sci. Eng. A 577 64-101
[7]  
Zeren M(2014)The ambient and high temperature deformation behavior of Al–Si–Cu–Mg alloy with minor Ti, Zr, Ni additions Mater. Des. 58 89-366
[8]  
Ibrahim MI(1995)Effect of iron in Al–Si casting alloys: a critical review (95–110) Trans. Am. Foundrymen’s Soc. 103 361-4132
[9]  
Samuel AM(2009)Three-dimensional study of Ni aluminides in an AlSi Acta Mater. 57 4125-5698
[10]  
Doty HW(2010) alloy by means of light optical and synchrotron microtomography Mater. Sci. Eng. A 527 5691-50