Creep Durability of Ni-Base Single Crystal Superalloy Containing Pb Impurity

被引:0
|
作者
Takahide Horie
Kyoko Kawagishi
Yuji Takata
Tadaharu Yokokawa
Shinsuke Suzuki
Hiroshi Harada
机构
[1] Waseda University,Department of Applied Mechanics and Aerospace Engineering
[2] National Institute for Materials Science (NIMS),Department of Materials Science
[3] Waseda University,Kagami Memorial Institute for Materials Science and Technology
[4] Waseda University,undefined
[5] Superalloy Design Laboratory,undefined
关键词
D O I
暂无
中图分类号
学科分类号
摘要
The effect of Pb on the creep properties of Ni-base single crystal superalloy was evaluated and compared with the reference data of polycrystalline superalloys. Alloy variants containing 0.04 (no Pb added), 0.9, and 31 ppm of Pb were prepared, and creep tests under different temperatures and stresses (i.e., 800/735, 900/392, 1000/245, 1100/137, and 1150 °C/137 MPa) as well as microstructural observations were conducted. The initial microstructure, such as the γ′ size and volume fraction of γ′, and the γ/γ′ microstructure after the creep test, such as the extent of raft structure formation, were almost identical in all the alloy variants. Moreover, the extent of topologically close-packed or precipitate phase formation could not be correlated with the Pb content. Based on these results and those of the creep tests, it was concluded that Pb did not affect the creep rupture life. In single crystal superalloy, no grain boundary exists, and the results of the field-emission electron-probe microanalysis indicated that Pb was dispersed in the substrate and its segregation did not occur during the creep test. Thus, in contrast to the Ni-base polycrystalline superalloy, no negative effect of Pb on the creep properties of the Ni-base single crystal superalloy was detected.
引用
收藏
页码:2627 / 2641
页数:14
相关论文
共 50 条
  • [22] Anisotropic Oxidation Resistance in a Ni-Base Single Crystal Superalloy
    Latief, Fahamsyah H.
    Alrasheedi, Nashmi H.
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2015, 10 (03): : 2183 - 2193
  • [23] Laser epitaxial cladding of Ni-base single crystal superalloy
    Fujita, Yoshihiro
    Saida, Kazuyoshi
    Nishimoto, Kazutoshi
    ADVANCED WELDING AND MICRO JOINING / PACKAGING FOR THE 21ST CENTURY, 2008, 580-582 : 67 - +
  • [24] Creep-fatigue behaviour of single-crystal Ni-base superalloy CMSX-8
    Rodas, Ernesto A. Estrada
    Gorgannejad, Sanam
    Neu, Richard W.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2019, 42 (09) : 2155 - 2171
  • [25] Simulation of very high temperature overheating during isothermal creep of single crystal Ni-base superalloy
    Cormier, Jonathan
    Milhet, Xavier
    Champion, Jean-Louis
    Mendez, Jose
    ADVANCED ENGINEERING MATERIALS, 2008, 10 (1-2) : 56 - 61
  • [26] Influence of heat treatment on anisotropic creep behavior of aluminide coating on a Ni-base single crystal superalloy
    Latief, F. H.
    Kakehi, K.
    MATERIALS & DESIGN, 2013, 52 : 134 - 142
  • [27] Effect of Sulfur on Creep Strength of Ni-Base Single-Crystal Superalloy, TMS-1700
    Joh, Yuichiro
    Utada, Satoshi
    Osawa, Makoto
    Kobayashi, Toshiharu
    Yokokawa, Tadaharu
    Kawagishi, Kyoko
    Suzuki, Shinsuke
    Harada, Hiroshi
    MATERIALS TRANSACTIONS, 2016, 57 (08) : 1305 - 1308
  • [28] A UNIQUE INFLUENCE OF CREEP DEFORMATION ON THE SUBSEQUENT FATIGUE CRACK PROPAGATION IN A SINGLE CRYSTAL NI-BASE SUPERALLOY
    Suzuki, Shiyu
    Sakaguchi, Motoki
    Inoue, Hirotsugu
    JOINT EPRI - 123HIMAT INTERNATIONAL CONFERENCE ON ADVANCES IN HIGH-TEMPERATURE MATERIALS, 2019, 2019, : 570 - 579
  • [29] Creep strength of yttrium doped 4th generation Ni-base single crystal superalloy
    Sato, Atsushi
    Sato, Akihiro
    Harada, Hiroshi
    Koizumi, Yutaka
    Kobayashi, Toshiharu
    Imai, Hachiro
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2006, 70 (04) : 380 - 383
  • [30] Isothermal oxidation behavior of single-crystal Ni-base superalloy containing rhenium in air
    Chunting, Liu
    Xiaofeng, Sun
    Ji, Ma
    Haiyan, Cong
    Wanfeng, Liu
    RARE METAL MATERIALS AND ENGINEERING, 2007, 36 (08) : 1407 - 1411