Mechanical properties and microstructural evolution of in-service Inconel 718 superalloy repaired by linear friction welding

被引:0
作者
M. Smith
L. Bichler
J. Gholipour
P. Wanjara
机构
[1] University of British Columbia – Okanagan School of Engineering,
[2] National Research Council of Canada,undefined
[3] Aerospace,undefined
来源
The International Journal of Advanced Manufacturing Technology | 2017年 / 90卷
关键词
Characterization; Inconel 718; Superalloy; In-service; Linear friction welding; Mechanical properties;
D O I
暂无
中图分类号
学科分类号
摘要
The focus of this study was to evaluate the possibility of extending the service life of an Inconel® alloy 718 (IN 718) aero-engine turbine using the linear friction welding (LFW) process. In particular, the repair of a blade integrated disk (BLISK) through replacement of blades damaged in-service was emulated by LFW virgin IN 718 to in-service IN 718. The virgin–in-service (V–IS) welds were then characterized to evaluate the evolution in the microstructural features, such as the grain size, δ phase, MC-type carbides and MN-type nitrides, across the weld region. In the as-welded condition, the weld and thermomechanically affected zones exhibited highly integral characteristics (i.e., no oxides, voids, or contamination), as well as no constitutional liquation of secondary phases (e.g., carbides and Laves phases). In the weld zone, grain refinement of the austenite (γ) matrix was observed, using electron back scattered diffraction (EBSD), and related to the occurrence of dynamic recrystallization during LFW. The microhardness and tensile mechanical properties of the weldments were investigated in the as-welded condition and compared to weldments with a standard post-weld heat treatment (PWHT). The results suggest that the LFW process is a promising technology for refurbishing IN 718 aero-engine components.
引用
收藏
页码:1931 / 1946
页数:15
相关论文
共 61 条
[1]  
Wang Y(2011)Hot deformation behavior of delta-processed superalloy 718 Material Science and Engineering A 528 3218-3227
[2]  
Shao W(2013)Microstructure and mechanical properties of friction welded alloy 718 Mater Sci Eng A 560 781-786
[3]  
Zhen L(2005)Linear friction welding of Ti-6Al-4V: processing, microstructure and mechanical property inter-relationships Metall Mater Trans A 36A 2149-2164
[4]  
Zhang B(2011)A study of linear friction weld microstructure in single crystal CMSX-486 superalloy Metall Mater Trans A 43A 921-933
[5]  
Damodaram R(2011)Analysis of microstructural changes induced by linear friction welding in a nickel-base superalloy Metall Mater Trans A 42A 3761-3777
[6]  
Raman S(2008)Multi-scale analysis of In-718 microstructure evolution during linear friction welding Adv Eng Mater 10 573-578
[7]  
Rao K(2007)Linear friction welding of In-718 process optimization and microstructure evolution Adv Mater Res 15-17 357-362
[8]  
Wanjara P(2013)Effect of post-weld heat treatments on microstructure and mechanical properties of friction welded alloy 718 joints Mater Des 53 954-961
[9]  
Jahazi M(2012)Suppressed liquation and microcracking in linear friction welded WASPALOY Mater Des 36 113-122
[10]  
Ola O(2011)Mechanical property and microstructure of linear friction welded WASPALOY Metall Mater Trans A 42A 729-744