A Preliminary Study of Deformation Behavior of Friction Stir Welded Ti-6Al-4V

被引:0
|
作者
Jiye Wang
Jianqing Su
Rajiv S. Mishra
Ray Xu
John A. Baumann
机构
[1] Missouri University of Science and Technology,Department of Materials Science and Engineering
[2] University of North Texas,Department of Materials Science and Engineering
[3] Rolls-Royce Corporation,undefined
[4] The Boeing Company,undefined
来源
Journal of Materials Engineering and Performance | 2014年 / 23卷
关键词
Friction stir welding; Titanium; Mechanical properties;
D O I
暂无
中图分类号
学科分类号
摘要
A preliminary study of deformation behavior of friction stir welded (FSW) Ti-6Al-4V was performed using two different tools with cylindrical and stepped spiral pin design for the welding process. The nugget regions experienced temperature above β transus and the matrix transformed to fine acicular α during cooling of the nugget. By using stepped spiral pin design, a local region with much refined grain structure and significant tool debris particles were observed. Room temperature tensile test showed increased strength and decreased ductility in the material from this region. Fractographic analysis revealed that tool debris particles served as void nucleation sites. Tensile tests of FSW material were carried out at 625 °C in the strain rates of 3 × 10−4 and 1 × 10−3 s−1. The strength was higher as compared to the as-received material. Microstructural evolution during tensile test was also investigated. Results showed that dynamic globularization occurred during the high temperature tensile test.
引用
收藏
页码:3027 / 3033
页数:6
相关论文
共 50 条
  • [21] Effects of intense cooling on microstructure and properties of friction-stir-welded Ti-6Al-4V alloy
    Liu, Zhenlei
    Wang, Yue
    Ji, Shude
    Li, Zhengwei
    MATERIALS SCIENCE AND TECHNOLOGY, 2018, 34 (02) : 209 - 219
  • [22] Effect of rotation speed on microstructure and mechanical properties of Ti-6Al-4V friction stir welded joints
    Zhou, L.
    Liu, H. J.
    Liu, Q. W.
    MATERIALS & DESIGN, 2010, 31 (05) : 2631 - 2636
  • [23] Achieving superior superplasticity from lamellar microstructure of a nugget in a friction-stir-welded Ti-6Al-4V joint
    Wu, L. H.
    Xiao, B. L.
    Ni, D. R.
    Ma, Z. Y.
    Li, X. H.
    Fu, M. J.
    Zeng, Y. S.
    SCRIPTA MATERIALIA, 2015, 98 : 44 - 47
  • [24] Fatigue and Static Properties of Built-up Friction Stir Welded Ti-6Al-4V I-Beams
    Sharma, Rahul
    Fick, Damon R.
    West, Michael K.
    Jasthi, Bharat K.
    MATERIALS PERFORMANCE AND CHARACTERIZATION, 2019, 8 (01)
  • [25] Microstructure and interface characterization of dissimilar friction stir welded lap joints between Ti-6Al-4V and AISI 304
    Campo, Kaio Niitsu
    Campanelli, Leonardo Contri
    Bergmann, Luciano
    dos Santos, Jorge Fernandez
    Bolfarini, Claudemiro
    MATERIALS & DESIGN, 2014, 56 : 139 - 145
  • [26] Fatigue performance of Friction Stir Welded Ti-6Al-4V subjected to various post weld heat treatment temperatures
    Edwards, P.
    Ramulu, M.
    INTERNATIONAL JOURNAL OF FATIGUE, 2015, 75 : 19 - 27
  • [27] Corrosion Behavior of Friction Stir-Processed and Gas Tungsten Arc-Welded Ti-6Al-4V
    Atapour, Masoud
    Pilchak, Adam L.
    Frankel, G. S.
    Williams, James C.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2010, 41A (09): : 2318 - 2327
  • [28] Peak temperatures during friction stir welding of Ti-6Al-4V
    Edwards, P.
    Ramulu, M.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2010, 15 (06) : 468 - 472
  • [29] Material flow during friction stir welding of Ti-6Al-4V
    Edwards, Paul D.
    Ramulu, M.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2015, 218 : 107 - 115
  • [30] Identification of Process Parameters for Friction Stir Welding Ti-6Al-4V
    Edwards, P.
    Ramulu, M.
    JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY-TRANSACTIONS OF THE ASME, 2010, 132 (03): : 0310061 - 03100610