Microstructure, mechanical properties and corrosion behavior of friction stir processed AA2014 alloy

被引:10
作者
Satyanarayana, M. V. N. V. [1 ]
Kumar, Adepu [2 ]
Jain, Vikram Kumar S. [3 ]
Kumar, Rahul [4 ]
Mishra, Sushil [4 ]
机构
[1] Anil Neerukonda Inst Technol & Sci, Visakhapatnam 531162, India
[2] Natl Inst Technol, Warangal 506004, India
[3] Natl Inst Technol, Trichy 620015, India
[4] Indian Inst Technol, Bombay 400076, India
关键词
Friction stir processing; Large-area stir zone; Microstructure and texture evolution; Mechanical properties; Work-hardening behavior; Corrosion; ALUMINUM-ALLOY; PARAMETERS; EVOLUTION;
D O I
10.1007/s43452-022-00565-8
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In the present study, a large-area stir zone (SZ) was fabricated in AA2014 alloy using multi-pass friction stir processing (FSP) with pin overlapping. The microstructure evolution, crystallographic texture, precipitation phenomenon, and tensile behavior were studied and reported. The microstructure of the large-area SZ consists of equiaxed fine grains with a high density of high angle boundaries caused by dynamic recovery (DRV) and continuous-dynamic recrystallization (C-DRX), and the grain refining has been uniform in each overlapping pass (the grain size within 4-7 mu m range). The material flow around the pin caused by the stirring action of the tool contributed to the creation of a strong Brass-{110} < 112 > and A-{110} < 111 > components in the first pass of SZ. Unlike first pass SZ, the second to fifth-pass SZ presents Copper-{112} < 111 > and Cube-{001} < 100 > components due to an increase of heat input by the shoulder to participate multiple times on each overlapping SZ. The hardness and strength of the FSP sample were found to be lowered relative to a base metal. Simultaneously, the SZ ductility increased after FSP by 155% due to the material softening and dissolution of Al2Cu precipitates in the SZ. Kocks-Mecking plots of the BM and FSP samples witnessed the Stage-III of work-hardening behavior. The fine-grain structure and precipitation phenomenon in the FSP sample resulted in better corrosion resistance than the base metal.
引用
收藏
页数:16
相关论文
共 39 条
[11]   LAWS FOR WORK-HARDENING AND LOW-TEMPERATURE CREEP [J].
KOCKS, UF .
JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY-TRANSACTIONS OF THE ASME, 1976, 98 (01) :76-85
[12]   Physics and phenomenology of strain hardening: the FCC case [J].
Kocks, UF ;
Mecking, H .
PROGRESS IN MATERIALS SCIENCE, 2003, 48 (03) :171-273
[13]   RELATION BETWEEN POLYCRYSTAL DEFORMATION AND SINGLE-CRYSTAL DEFORMATION [J].
KOCKS, UF .
METALLURGICAL TRANSACTIONS, 1970, 1 (05) :1121-&
[14]   Advancing towards constitutive equations for the metal industry via the LEDS theory [J].
Kuhlmann-Wilsdorf, D .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2004, 35A (02) :369-418
[15]   Mechanical properties of fine-grained aluminum alloy produced by friction stir process [J].
Kwon, YJ ;
Shigematsu, I ;
Saito, N .
SCRIPTA MATERIALIA, 2003, 49 (08) :785-789
[16]   MODIFIED STRESS-STRAIN RELATION FOR FCC METALS AND ALLOYS [J].
LUDWIGSON, DC .
METALLURGICAL TRANSACTIONS, 1971, 2 (10) :2825-+
[17]   Recrystallization mechanisms during friction stir welding/processing of aluminum alloys [J].
McNelley, T. R. ;
Swaminathan, S. ;
Su, J. Q. .
SCRIPTA MATERIALIA, 2008, 58 (05) :349-354
[18]   Friction stir welding and processing [J].
Mishra, RS ;
Ma, ZY .
MATERIALS SCIENCE & ENGINEERING R-REPORTS, 2005, 50 (1-2) :1-78
[19]   Recent advances in friction-stir welding - Process, weldment structure and properties [J].
Nandan, R. ;
DebRoy, T. ;
Bhadeshia, H. K. D. H. .
PROGRESS IN MATERIALS SCIENCE, 2008, 53 (06) :980-1023
[20]   Effect of Friction Stir Processing on Pitting Corrosion and Intergranular Attack of 7075 Aluminum Alloy [J].
Navaser, M. ;
Atapour, M. .
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2017, 33 (02) :155-165