Crack Resistance of Welded Joints of Pipe Steels of Strength Class K60 of Different Alloying Systems

被引:0
作者
T. I. Tabatchikova
N. A. Tereshchenko
I. L. Yakovleva
A. N. Makovetskii
S. V. Shander
机构
[1] M. N. Mikheev Institute of Metal Physics of the Ural Branch of the Russian Academy of Sciences,
[2] Chelyabinsk Pipe-Rolling Plant,undefined
[3] JSC,undefined
来源
Metal Science and Heat Treatment | 2018年 / 59卷
关键词
pipe steel; welded joint; heat-affected zone; weld; crack resistance; size of austenite grains; bainite morphology;
D O I
暂无
中图分类号
学科分类号
摘要
The crack resistance of welded joints of pipe steels of strength class K60 and different alloying systems is studied. The parameter of the crack tip opening displacement (CTOD) is shown to be dependent on the size of the austenite grains and on the morphology of bainite in the superheated region of the heat-affected zone of the weld. The crack resistance is shown to be controllable due to optimization of the alloying system.
引用
收藏
页码:767 / 772
页数:5
相关论文
共 4 条
[1]  
Gorkunov ES(2014)Effect of the structure and stress state on the magnetic properties of metal in different zones of welded large-diameter pipes Fiz. Met. Metalloved. 115 1011-1019
[2]  
Zadvorkin SM(undefined)undefined undefined undefined undefined-undefined
[3]  
Putilova EA(undefined)undefined undefined undefined undefined-undefined
[4]  
Savray RA(undefined)undefined undefined undefined undefined-undefined