Effect of Cold Working on Hot Corrosion Behavior of 9 Cr–1 Mo Ferritic Steel in 75 wt% Na2SO4 + 25 wt% K2SO4 Molten Salt Environment at 900 °C

被引:0
|
作者
Amarish K. Shukla
Dinesh Gond
D. Puri
机构
[1] Central Institute of Plastics Engineering and Technology,Metallurgical & Materials Engineering Department
[2] Indian Institute of Technology Roorkee,HEEP
[3] Bharat Heavy Electricals Limited,undefined
关键词
Cold work; Air oxidation; Hot corrosion; 9 Cr–1 Mo ferritic steel;
D O I
暂无
中图分类号
学科分类号
摘要
The hot corrosion behavior of as received (0 %), 10, 30 and 50 % cold rolled T-91 (9 Cr–1 Mo) ferritic steels has been studied in salt 75 wt% Na2SO4 + 25 wt% K2SO4 atmosphere under cyclic heating conditions at a temperature of 900 °C for 50 cycles. Each cycle consisted of 1 h heating at 900 °C followed by 20 min of cooling in air. Oxidation kinetics was studied using thermogravimetric technique by recording the weight gain at the end of each cycle. Oxidation kinetics of cold rolled sample with 10 and 50 % reduction followed parabolic rate law while cold-worked with 30 % showed accelerated rate of weight gain compared to the other cold worked samples as well as un-worked sample. 30 % cold worked sample in salt atmosphere was fully oxidized after 50 cycles and only fragmented thick scale remained. X-ray diffraction and scanning electron microscopy were utilized for characterizing the oxide layer. Cold rolled steel sample with 10 % was found to be more oxidation resistant compared to other cases.
引用
收藏
页码:1049 / 1057
页数:8
相关论文
共 50 条
  • [41] Prediction modeling of Type-I hot corrosion performance of Ti-Al-Mo-X (X=Cr, Mn) alloys in (Na, K)2SO4 molten salt mixture environment at 900°C
    Garip, Y.
    Garip, Z.
    Ozdemir, O.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 843
  • [42] The effect of pre-oxidation on the hot corrosion behavior of CoNiCrAlHf alloy in Na2SO4 environment at elevated temperature
    Rawaid Ali
    Peng Song
    Muhammad Khan
    Taihong Huang
    Shabir Ali
    Syed Hatim Sha
    Jiansheng Lu
    Zain Ul Wahab
    Seemab Pervaiz
    Applied Physics A, 2022, 128
  • [43] The effect of pre-oxidation on the hot corrosion behavior of CoNiCrAlHf alloy in Na2SO4 environment at elevated temperature
    Ali, Rawaid
    Song, Peng
    Khan, Muhammad
    Huang, Taihong
    Ali, Shabir
    Sha, Syed Hatim
    Lu, Jiansheng
    Ul Wahab, Zain
    Pervaiz, Seemab
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2022, 128 (09):
  • [44] Aluminizing and boroaluminizing treatments of Mar-M247 and their effect on hot corrosion resistance in Na2SO4−NaCl molten salt
    J. H. Cho
    T. W. Kim
    K. S. Son
    J. H. Yoon
    H. S. Kim
    G. G. Leisk
    D. B. Mitton
    R. M. Latanision
    Metals and Materials International, 2003, 9 : 303 - 310
  • [45] Hot Corrosion Resistance of CeO2-Doped Cr3C2–NiCr Coatings on Austenite Steel Against Molten Salt (Na2SO4–60%V2O5) Environment
    Singh H.
    Chatha S.S.
    Sidhu B.S.
    Journal of Bio- and Tribo-Corrosion, 2023, 9 (01)
  • [46] HOT CORROSION OF NICKEL IN NA2SO4-CASO4-PBO SALT MIXTURES AT 900-DEGREES-C
    SHATYNSKI, SR
    ARBAB, M
    JOURNAL OF METALS, 1980, 32 (12): : 5 - 5
  • [47] Raman spectral quantification of Li2SO4, Na2SO4, K2SO4 and Cs2SO4 at 25 to 250 °C and its potential implications for the determination of sulfate contents in natural fluid inclusions
    Chen, Chen
    Shang, Linbo
    Zhou, Yunhe
    Jiang, Ziqi
    Wang, Xinsong
    Chou, I-Ming
    Li, Jianguo
    Wang, Zhenglong
    ORE GEOLOGY REVIEWS, 2024, 168
  • [48] CORROSION BEHAVIOR OF NIMONIC-75 AND NI-19.4CR-1.25AL IN NACL AND NA2SO4
    KAMESWARI, S
    MISRA, RDK
    WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1987, 38 (01): : 20 - 25
  • [49] Hot Corrosion of Cobalt-Based Alloy with (Na, K)2SO4 Coating At 900 °C
    Fu, Guangyan
    Zhao, Xin
    Liu, Qun
    Su, Yong
    ADVANCED ENGINEERING MATERIALS, PTS 1-3, 2011, 194-196 : 1305 - 1308
  • [50] Hot corrosion behavior and near-surface microstructure of a "low-temperature high-activity Cr-aluminide" coating on inconel 738LC exposed to Na2SO4, Na2SO4 + V2O5 and Na2SO4 + V2O5 + NaCl at 900 °C
    Doolabi, M. Salehi
    Ghasemi, B.
    Sadrnezhaad, S. K.
    Habibollahzadeh, A.
    Jafarzadeh, K.
    CORROSION SCIENCE, 2017, 128 : 42 - 53