Microstructural and mechanical response of SiC and TiO2 particles reinforced friction stir welded AA7075 and AA2024

被引:0
作者
Pradeep Kumar Mouria
Ranganath M. Singari
Reeta Wattal
机构
[1] Delhi Technological University,Department of Mechanical Engineering
[2] Manav Rachna University,Department of Mechanical Engineering
来源
International Journal on Interactive Design and Manufacturing (IJIDeM) | 2024年 / 18卷
关键词
Friction stir welding; Nanoparticles; Microstructure; EDX; Tensile test; Hardness;
D O I
暂无
中图分类号
学科分类号
摘要
The main objective of this study is the microstructure and mechanical properties of AA7075 and AA2024 welded joints when friction stir welded with different reinforced materials (SiC and TiO2). The imperfection-free welds are portrayed by great mechanical blending between AA7075 and AA2024 and good, reinforced material dispensation in the stir zone. Grain refinement of weld with reinforced material is compared with weld without reinforced material. It is also observed that double-pass processed welds have coarser microstructure than a single pass. Scanning electron microscopy is used to analyze the size and distribution of reinforced particles in the various zones of the weld. The maximum tensile strength of the joint produced with SiC reinforcement particles is 206 MPa, while the minimum tensile strength (177 MPa) was observed without reinforcement particles. A comparative study has been carried out between the friction stir welding of AA7075 and AA2024 with TiO2 and SiC reinforced material and with unreinforced material. The nanoparticles disperse within the weld zone, leading to a refined microstructure and preventing the formation of detrimental defects. This dispersion improves load-bearing capabilities, effectively increasing the tensile strength of the joint. The nanoparticles contribute to a more uniform distribution of stresses and help mitigate crack initiation and propagation. The average hardness value at the stir zone with SiC and TiO2 nanoparticles was observed as 172 HV and 164 HV, respectively, while the minimum hardness value of 147 HV was observed without nanoparticles.
引用
收藏
页码:1331 / 1343
页数:12
相关论文
共 168 条
[1]  
Zhao X(2011)Weld quality improvement with hybrid FSW technology assisted by preheating for copper T2/aluminium 5A06 dissimilar materials Appl. Mech. Mater. 121–126 1707-1711
[2]  
Dong FB(2013)Ac ce p te t J. Mater. Process. Tech. 17 539-544
[3]  
Su GY(2012)Investigation of weld defects in dissimilar friction stir welding of aluminium to brass by radiography Sci. Technol. Weld. Join. 17 581-588
[4]  
Guo LJ(2012)Effect of materials position on friction stir lap welding of Al to Cu Sci. Technol. Weld. Join. 32 285-295
[5]  
Galvão I(2023)Modification of microstructure and mechanical properties of aa6082/zrb2 processed by multipass friction stir processing J. Mater. Eng. Perform. 236 162-175
[6]  
Verdera D(2016)Fatigue of alclad AA2024-T3 swept friction stir spot welds in cross-tension specimens J. Mater. Process. Technol. 25 1779-1786
[7]  
Gesto D(2015)Microstructure and mechanical properties of dissimilar Al–Cu joints by friction stir welding Trans. Nonferrous Met. Soc. China 37 2484-2502
[8]  
Loureiro A(2022)Effect of material positioning on Si-rich TIG welded joints of AA6082 and AA8011 by friction stir processing J. Adhes. Sci. Technol. 2 41-46
[9]  
Rodrigues DM(2017)Microstructure and mechanical properties in nano and microscale SiC-included dissimilar friction stir welding of AA6061-AA2024 Mater. Sci. Technol. 45 1635-1639
[10]  
Esmaeili A(2017)Mechanical characterization of SA-508Gr3 and SS-304L steel weldments Int. J. Adv. Prod. Ind. Eng. 25 2833-2846