Transient liquid phase bonding of HfC-based ceramics

被引:0
作者
Laura Esposito
Diletta Sciti
Laura Silvestroni
Cesare Melandri
Stefano Guicciardi
Noritaka Saito
Kunihiko Nakashima
Andreas M. Glaeser
机构
[1] CNR-ISTEC,Department of Materials Science and Engineering
[2] Institute of Science and Technology for Ceramics,Department of Materials Science and Engineering
[3] CNR-ISMAR,undefined
[4] Kyushu University,undefined
[5] University of California,undefined
来源
Journal of Materials Science | 2014年 / 49卷
关键词
Reaction Layer; Transient Liquid Phase; Isothermal Solidification; Bond Region; Indentation Modulus;
D O I
暂无
中图分类号
学科分类号
摘要
Transient liquid phase (TLP) bonding enables joining at lower temperatures than traditional bonding techniques and preserves the potential for high-temperature applications, making it particularly attractive for joining ultra-high-temperature ceramics (UHTCs) such as carbides and borides. The feasibility of a TLP joint between “pure” carbides has been recently demonstrated. The present study examines the interactions that occur between undoped HfC or MoSi2-doped HfC and a Ni/Nb/Ni multilayer interlayer during TLP bonding. Bonding is performed at 1400 °C for 30 min in a high-vacuum furnace. SEM–EDS characterization shows that the reaction layer formed at the interlayer/ceramic interface contains mixed carbides and depending upon the ceramic, Ni–Nb–Hf, or Ni–Nb–Hf–Si, or Ni–Nb–Si alloys. Nanoindentation tests traversing the reaction layer between the bulk ceramic and Nb foil midplane also show a clear transition zone across which the indentation modulus and hardness vary. Crack-free joints have been obtained with undoped HfC. The addition of 5 vol% MoSi2 introduces small (<5 μm long) isolated cracks within the reaction layer, whereas with 15 vol% MoSi2 added, cracking was pervasive within the reaction layer. When the reaction layer exceeds a critical thickness, as in the case of the bond obtained with HfC doped with 15 vol% MoSi2, residual stresses become sufficiently large to cause extensive cracking and bond failure. The results suggest a need to characterize and balance the positive role of additives on sintering with the potentially deleterious role they may have on joining.
引用
收藏
页码:654 / 664
页数:10
相关论文
共 119 条
[1]  
Opeka MM(2004)Diffusion of nickel in niobium J Mater Sci 39 5887-427
[2]  
Talmy IG(1982)Hydrogen absorption in Nb J Nucl Mater 105 331-undefined
[3]  
Zaykoski JA(2012)CoSi and Nb J Renew Sustain Energy 4 033104-undefined
[4]  
Ogawa T(1961)NiSi Archiv für das Eisenhüttenvesen 6 421-undefined
[5]  
Ikawa K(2009)undefined J Aerosp Eng 233 1153-undefined
[6]  
Sani E(2012)undefined J Eur Ceram Soc 32 1795-undefined
[7]  
Mercatelli L(2012)undefined Int J Sci Emerg Technol 3 31-undefined
[8]  
Sansoni P(2010)undefined Adv Mater Sci Eng 11 835018-undefined
[9]  
Silvestroni L(2008)undefined J Eur Ceram Soc 28 1899-undefined
[10]  
Sciti D(2012)undefined J Eur Ceram Soc 32 4469-undefined