Size effect on fracture behavior of quasi-brittle materials during uniaxial compression tests

被引:0
作者
Junjie Wang
Chuan Lv
Shiyuan Huang
Zhenfeng Qiu
机构
[1] Chongqing Jiaotong University,School of Materials Science and Engineering
[2] Chongqing Jiaotong University,Engineering Research Center of Diagnosis Technology and Instruments of Hydro
[3] Chongqing Jiaotong University,Construction
来源
Archive of Applied Mechanics | 2023年 / 93卷
关键词
Size effect; Uniaxial compression test; Fracture behavior; Fracture process zone;
D O I
暂无
中图分类号
学科分类号
摘要
Understanding the size dependence of quasi-brittle materials' fracture behavior is useful in assessing the safety of flawed rock engineering structures. In this study, a set of uniaxial compression tests were conducted to scrutinize the mechanical properties and crack morphology of cubic specimens with sizes of 75 mm, 100 mm, 125 mm and 150 mm. The results showed that the specimens had significant size dependence in terms of strength and crack initiation angle. The crack type and fracture pattern were not affected by the specimen size and were mainly controlled by the pre-existing crack inclination angle. Next, the test results were compared with the maximum tangential stress criterion considering the T-stress. The results also showed that the crack initiation angles of specimens with different sizes were in good agreement with the theoretical calculations. The non-singular compressive stress perpendicular to the crack surface inhibited the generation of the fracture process zone (FPZ). In addition, the stress required for tensile failure was smaller for large-size specimens, leading to a decrease in the length of the FPZ with increasing specimen size. The FPZ variation law of the uniaxial compression tests was greatly different from that of the mode I loading.
引用
收藏
页码:3171 / 3188
页数:17
相关论文
共 139 条
  • [21] Kuruppu MD(1978)Combined mode fracture toughness measurement by the disk test J. Eng. Mater. Technol. 66 79-2499
  • [22] Aliha MRM(2002)Measurement of rock fracture toughness under modes I and II and mixed-mode conditions by using disc-type specimens Eng. Geol. 240 107365-1845
  • [23] Ayatollahi MR(2020)Quasi-static loading rate effects on fracture process zone development of mixed-mode (I-II) fractures in rock-like materials Eng. Fract. Mech. 168 227-52
  • [24] Smith DJ(2011)Strength failure and crack coalescence behavior of brittle sandstone samples containing a single fissure under uniaxial compression Int. J. Fract. 204 319-14
  • [25] Zhang S(2018)Fracture analysis of sandstone with a single filled flaw under uniaxial compression Eng. Fract. Mech. 49 2482-6
  • [26] An D(2012)Influence of flaw inclination angle and loading condition on crack initiation and propagation Int. J. Solids Struct. 76 1833-525
  • [27] Zhang X(2009)Experimental study on mechanical behavior of brittle marble samples containing different flaws under uniaxial compression Eng. Fract. Mech. 14 40-114
  • [28] Bažant ZP(2014)A bonded particle model for analysis of the flaw orientation effect on crack propagation mechanism in brittle materials under compression Arch. Civ. Mech. Eng. 49 1-351
  • [29] Gettu R(2016)The effects of crack openings on crack initiation, propagation and coalescence behavior in rock-like materials under uniaxial compression Rock Mech. Rock Eng. 49 1-241
  • [30] Kazemi MT(2016)Strength of rock-like specimens with pre-existing cracks of different length and width Rock Mech. Rock Eng. 274 108795-150