Influence of isothermal aging in LDX 2101 duplex stainless steel on the microstructure and local properties

被引:0
作者
Naima Ouali
Billel Cheniti
Brahim Belkessa
Bouzid Maamache
Ramdhane Kouba
Maamar Hakem
机构
[1] Research Center in Industrial Technologies CRTI,Laboratoire de Technologie des Matériaux, Département SDM, Faculté de Génie Mécanique et Génie des Procédés
[2] USTHB,undefined
来源
The International Journal of Advanced Manufacturing Technology | 2021年 / 116卷
关键词
Microstructure; Interface; Precipitates; Nano-hardness; Surface degradation;
D O I
暂无
中图分类号
学科分类号
摘要
In the present work, the interface morphology and the evolution of nitride precipitates in LDX 2101 stainless steel isothermally treated at 750 °C for various aging times were investigated. The microstructure results showed that the Cr2N nitrides precipitated along the δ/γ interface with 200 nm in length and continue to grow to 2 μm after 240 h of aging. However, only Cr2N nitrides were found at the δ/δ interface after long term of aging. Atomic force microscopy (AFM) analysis revealed that Cr2N nitrides and Cr23C6 carbides started to precipitate after the first 10 min of aging with a small needle shape of the former and specific triangular morphology of the latter. The evolution of hardness and Young’s modulus of the interfaces, performed with nano-indentation measurements, showed that the δ/γ interface became harder (4.1 ± 0.2 GPa) with increasing aging times, whereas negligible changes in the hardness and elastic modulus were recorded at the δ/δ interface. 3D topographic analysis of the immersed surfaces revealed that the susceptibility of δ phase to preferential dissolution in 3.5% NaCl solution increased with aging time. This behavior was manifested by the important imperfections of δ phase, the high surface roughness (55.7 nm), and the deep corrosion pits (30 nm) along the δ/γ interface and around the Cr2N nitrides.
引用
收藏
页码:1881 / 1893
页数:12
相关论文
共 168 条
  • [11] Choi JY(2009)Electrochemical impedance spectroscopy (EIS) as a tool for measuring corrosion of polymer-coated fasteners used in treated wood For Prod J 59 77-82
  • [12] Ji JH(2012)Effect of surface texturing on friction properties of WC / Co cemented carbide Mater Des 41 142-149
  • [13] Hwang SW(2019)Effect of heat input on microstructure, residual stress, and corrosion resistance of UNS 32101 lean duplex stainless steel weld joints J Mater Eng Perform 28 4252-4264
  • [14] Park KT(2000)Formation of core / rim structures in Ti ( C , N ) -WC-Ni cermets via a dissolution and pricipitation process J Am Ceram Soc 83 1489-1494
  • [15] Breda M(2006)Fracture toughness of the lean duplex stainless steel LDX 2101 Metall Mater Trans A Phys Metall Mater Sci 37 2975-2981
  • [16] Pellizzari M(2016)Pitting corrosion susceptibility of friction stir welded lean duplex stainless steel joints Int J Adv Manuf Technol 83 721-728
  • [17] Frigo M(2010)Study of nobility of chromium nitrides in isothermally aged duplex stainless steels by using SKPFM and SEM/EDS Corros Sci 52 179-186
  • [18] Silva R(1993)Influence of isothermal phase transformations on toughness and pitting corrosion of super duplex stainless steel SAF 2507 Mater Sci Technol (UK) 9 545-554
  • [19] Baroni LFS(2009)Effect of ageing on precipitation and impact energy of 2101 economical duplex stainless steel Mater Charact 60 50-55
  • [20] Silva MBR(2021)Effect of aging temperature on the microstructure, local mechanical properties, and wear behavior of a UNS S32750 super duplex stainless steel J Mater Eng Perform 30 546-555