Improvement of the corrosion behavior of AISI 304L stainless steel by deep rolling treatment under cryogenic cooling

被引:0
|
作者
Khouloud Gharbi
Naoufel Ben Moussa
Amir Ben Rhouma
Nabil Ben Fredj
机构
[1] Université de Tunis,Laboratoire de Mécanique, Matériaux et Procédés (LR99ES05), ENSIT
来源
The International Journal of Advanced Manufacturing Technology | 2021年 / 117卷
关键词
Deep rolling; Cryogenic cooling; AISI 304L stainless steel; Deep rolling speed; Corrosion behavior;
D O I
暂无
中图分类号
学科分类号
摘要
The effects of deep rolling parameters, particularly, work speed and cooling conditions (dry and cryogenic) on the surface integrity of AISI 304L machined samples and their further impact on uniform and localized corrosion behavior in chloride environment were experimentally investigated in this work. The electrochemical behavior of machined and deep rolled samples was assessed using cyclic potentiodynamic polarization tests in synthetic seawater. It was found that the corrosion behavior of AISI 304L deep rolled components is related to combined factors: surface roughness, recrystallized grains, strain-induced martensite, microhardness and residual stresses. Findings of this study exhibit that grain refinement generated in the surface layers leads to improved corrosion behavior of deep rolled specimens with regard to machining state. In addition, samples deep rolled at a speed of 25 m/min, without cooling, showed better corrosion resistance than those processed under cryogenic cooling. However, the application of cryogenic deep rolling at speeds of 75 and 120 m/min significantly enhanced the electrochemical behavior of mechanically treated specimens. Despite of high amounts of strain-induced martensite that can deteriorate the electrochemical behavior, it was shown that specimens deep rolled under these conditions, presenting better surface characteristics, depicted an improved corrosion resistance.
引用
收藏
页码:3841 / 3857
页数:16
相关论文
共 50 条
  • [21] Effect of heat treatment on corrosion behavior of laser surface melted 304L stainless steel
    Istanbul Univ, Istanbul, Turkey
    Mater Sci Eng A Struct Mater Prop Microstruct Process, 1-2 (324-331):
  • [22] Effects of aging time on intergranular and pitting corrosion behavior of Cu-bearing 304L stainless steel in comparison with 304L stainless steel
    Jiang, Jie
    Xu, Dake
    Xi, Tong
    Shahzad, M. Babar
    Khan, M. Saleem
    Zhao, Jinlong
    Fan, Xinmin
    Yang, Chunguang
    Gu, Tingyue
    Yang, Ke
    CORROSION SCIENCE, 2016, 113 : 46 - 56
  • [23] WEAR PERFORMANCE OF AISI 304L STAINLESS STEEL UNDER VARIOUS AMBIENT TEMPERATURES
    Karabeyoglu, S.
    Eksi, O.
    Ergene, B.
    Bolat, C.
    LATIN AMERICAN APPLIED RESEARCH, 2022, 52 (04) : 289 - 296
  • [24] Evolutions of mechanical properties of AISI 304L stainless steel under shear loading
    Zergani, Aqil
    Mirzadeh, Hamed
    Mahmudi, Reza
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 791
  • [25] Corrosion degradation of AISI type 304L stainless steel for application in nuclear reprocessing plant
    Ningshen, S.
    Sakairi, M.
    JOURNAL OF SOLID STATE ELECTROCHEMISTRY, 2015, 19 (12) : 3533 - 3542
  • [26] Microstructural investigation on strengthening mechanisms of AISI 304L austenitic stainless steel during cryogenic deformation
    Behjati, P.
    Najafizadeh, A.
    Kermanpur, A.
    MATERIALS SCIENCE AND TECHNOLOGY, 2011, 27 (12) : 1828 - 1832
  • [28] Erosion-Corrosion of AISI 304L Stainless Steel Affected by Industrial Copper Tailings
    Soliz, Alvaro
    Caceres, Luis
    Pineda, Fabiola
    Galleguillos, Felipe
    METALS, 2020, 10 (08) : 1 - 16
  • [29] The Effect of Severe Plastic Deformation on the Corrosion Resistance of AISI Type 304L Stainless Steel
    Gopinath Shit
    S. Ningshen
    Journal of Materials Engineering and Performance, 2020, 29 : 5696 - 5709
  • [30] The Effect of Severe Plastic Deformation on the Corrosion Resistance of AISI Type 304L Stainless Steel
    Shit, Gopinath
    Ningshen, S.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (09) : 5696 - 5709